Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1180 - 1250 MPa | 171000 - 181000 psi | |
Plansee DENAL® 920 60 20 Tungsten-Nickel-Iron-Cobalt Alloy Characteristics:exceptionally stronghigh densityoutstanding mechanical damping capabilitiesHigh absorption of X-ray and gamma radiationInformation provided by Plansee. |
|||
Tensile Strength, Yield | 1030 - 1250 MPa | 149000 - 181000 psi | |
Materion Beryllium Copper Alloy 190 Strip; XHMS (TM08) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 69%Formability Ratio, 90° Bend, R.. |
|||
Tensile Strength, Yield | 890 - 1250 MPa | 129000 - 181000 psi | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 51 to 76 mm Thickness (UNS C17200) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Yield | 990 - 1250 MPa | 144000 - 181000 psi | |
Materion Beryllium Copper Alloy 25 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: 3 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed i.. |
|||
Tensile Strength, Yield | 990 - 1250 MPa | 144000 - 181000 psi | |
Materion Beryllium Copper Alloy M25 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: 3 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed i.. |
|||
Tensile Strength, Yield | 1100 - 1250 MPa | 160000 - 181000 psi | Solution Annealed & Aged |
Materion Beryllium Nickel M220C Information supplied by Brush Wellman Engineered Materials.Brush M220C is characterized by high levels of strength, hardness, and thermal conductivity combined with excellent resistance to wear, cor.. |
|||
Tensile Strength, Yield | 950 - 1250 MPa @Strain 0.200 % |
138000 - 181000 psi @Strain 0.200 % |
|
SSAB Tunnplat Docol® 1200 DP High-strength Steel The steels are annealed at temperatures between 750°C and 850°C, depending on the grade of steel, and then are hardened by quenching in water. Tempering is the next stage, in which the steel .. |