Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 22.0 - 120 MPa | 3190 - 17400 psi | Average value: 57.4 MPa Grade Count:244 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Tensile Strength, Yield | 47.1 - 120 MPa | 6830 - 17400 psi | Average value: 94.9 MPa Grade Count:48 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Tensile Strength, Yield | 45.0 - 120 MPa | 6530 - 17400 psi | Average value: 82.5 MPa Grade Count:26 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Tensile Strength, Yield | 44.0 - 120 MPa | 6380 - 17400 psi | Average value: 55.2 MPa Grade Count:14 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |