Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1172 - 1179 MPa @Strain 0.200 % |
170000 - 171000 psi @Strain 0.200 % |
|
Latrobe Lescalloy® UT-18 VAC-ARC ; 3.25 in. round High Strength Alloy Steel UT-18 VAC-ARC is a medium-carbon, low-alloy heat resistant steel having high strength to 1000°F. It is used primarily for turbine and compressor rotor shafts. Vacuum consumable electrode melting.. |