Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1165 - 1172 MPa @Strain 0.200 % |
169000 - 170000 psi @Strain 0.200 % |
|
Latrobe Lescalloy® UT-18 VAC-ARC ; 3.75 in. round High Strength Alloy Steel UT-18 VAC-ARC is a medium-carbon, low-alloy heat resistant steel having high strength to 1000°F. It is used primarily for turbine and compressor rotor shafts. Vacuum consumable electrode melting.. |
|||
Tensile Strength, Yield | 1145 - 1172 MPa @Strain 0.200 % |
166100 - 170000 psi @Strain 0.200 % |
|
Latrobe Lescalloy® UT-18 VAC-ARC ; 4 in. round High Strength Alloy Steel UT-18 VAC-ARC is a medium-carbon, low-alloy heat resistant steel having high strength to 1000°F. It is used primarily for turbine and compressor rotor shafts. Vacuum consumable electrode melting.. |
|||
Tensile Strength, Yield | 793 - 1172 MPa | 115000 - 170000 psi | |
Materion Beryllium Nickel Strip - Alloy 360 1/2 Hard Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0.7Formability Ratio (bad Way).. |
|||
Tensile Strength, Yield | 1138 - 1172 MPa @Strain 0.200 % |
165100 - 170000 psi @Strain 0.200 % |
Core heat treated from 1850°F |
Latrobe CBS-223â„¢ VIM-VAR Carburizing Bearing and Gear Steel CBS-223 VIM-VAR steel is a double vacuum melted carburizing steel with high hot hardness characteristics. Double vacuum melting sequentially combines vacuum induction melting with VACARCâ„¢ remel.. |