Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 850 - 1050 MPa | 123000 - 152000 psi | Swaged after Sintering |
MarkeTech 95-3-2 Tungsten Alloy, AMS-T-21014 Class 3 Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st.. |
|||
Tensile Strength, Yield | 800 - 1050 MPa | 116000 - 152000 psi | Swaged after Sintering |
MarkeTech 96-3-1 Tungsten Alloy, AMS-T-21014 Class 3 Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st.. |
|||
Tensile Strength, Yield | 750 - 1050 MPa | 109000 - 152000 psi | Swaged after Sintering |
MarkeTech 97-2-1 Tungsten Alloy, AMS-T-21014 Class 4 Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st.. |
|||
Tensile Strength, Yield | 931 - 1050 MPa | 135000 - 153000 psi | |
Materion Alloy 390 Beryllium Nickel Strip Alloy 390 was specifically designed for high power applications, providing a unique combination of high strength and high conductivity. Increasing power requirements are driving the need for lower c.. |