Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 5.60 - 10.4 MPa | 812 - 1510 psi | ±30% change after 168 hours @ 70°C; ASTM D412 |
Precision Polymer Engineering R90B Natural Rubber Natural Rubber, 85-95 °IRHD. This material is based on high-quality plantation (Hevea) rubber, reinforced with carbon black.Applications: Natural rubber offers low compression set, high tensile st.. |