Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 990 - 1280 MPa | 144000 - 186000 psi | |
Materion Beryllium Copper Alloy 165 Rod and Bar; HT (TH04) Temper; over 9.5 to 25.4 mm (UNS C17000) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Tensile Strength, Yield | 990 - 1280 MPa | 144000 - 186000 psi | |
Materion Beryllium Copper Alloy 165 Rod and Bar; HT (TH04) Temper; up to 9.5 mm (UNS C17000) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Tensile Strength, Yield | 990 - 1320 MPa | 144000 - 191000 psi | |
Materion Beryllium Copper Alloy 25 Rod and Bar; HT (TH04) Temper; over 25.4 to 76 mm (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Tensile Strength, Yield | 990 - 1320 MPa | 144000 - 191000 psi | |
Materion Beryllium Copper Alloy 25 Tube; HT (TH04) Temper; 0ver 25.4 to 76 mm o.d. (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Tensile Strength, Yield | 990 - 1250 MPa | 144000 - 181000 psi | |
Materion Beryllium Copper Alloy 25 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: 3 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed i.. |
|||
Tensile Strength, Yield | 990 - 1210 MPa | 144000 - 175000 psi | |
Materion Beryllium Copper Alloy M25 Rod and Bar; AT (TF00) Temper; up to 76 mm (UNS C17300) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Tensile Strength, Yield | 990 - 1320 MPa | 144000 - 191000 psi | |
Materion Beryllium Copper Alloy M25 Rod and Bar; HT (TH04) Temper; over 25.4 to 76 mm (UNS C17300) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Tensile Strength, Yield | 990 - 1250 MPa | 144000 - 181000 psi | |
Materion Beryllium Copper Alloy M25 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: 3 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed i.. |
|||
Tensile Strength, Yield | 990 - 1210 MPa | 144000 - 175000 psi | |
Materion Beryllium Copper Alloy 25 Rod and Bar; AT (TF00) Temper; up to 76 mm (UNS C17200) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Tensile Strength, Yield | 990 - 1210 MPa | 144000 - 175000 psi | |
Materion Beryllium Copper Alloy 25 Tube; AT (TF00) Temper; up to 76 mm o.d. (UNS C17200) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Tensile Strength, Yield | 990 MPa | 144000 psi | |
SSAB Tunnplat Domex® 024 BOR Oil quenched Boron Steel Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron .. |