Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 940 MPa @Strain 0.200 % |
136000 psi @Strain 0.200 % |
|
Haynes 25 alloy, cold worked sheet, 15% cold reduction, aged at 370°C (700°F) for 1 hour Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | 940 MPa @Temperature 23.0 °C |
136000 psi @Temperature 73.4 °F |
0°, Conditioning: 23°C; ASTM D3039 |
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, HTA Fiber Designation: C193PW, Plain weaveInformation provided by HexCel |
|||
Tensile Strength, Yield | >= 940 MPa @Strain 0.200 % |
>= 136000 psi @Strain 0.200 % |
|
CLAL-MSX DECLAFOR® 1015 THX Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |