Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 915 MPa @Strain 0.200 % |
133000 psi @Strain 0.200 % |
|
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Tensile Strength, Yield | 915 MPa @Strain 0.200 %, Temperature 540 °C |
133000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes 25 alloy, cold worked sheet, 20 % cold reduction Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |