Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 900 - 1100 MPa | 131000 - 160000 psi | Swaged after Sintering |
MarkeTech 91-6-3 Tungsten Alloy, AMS-T-21014 Class 1 Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st.. |
|||
Tensile Strength, Yield | 900 - 1100 MPa | 131000 - 160000 psi | Swaged after Sintering |
MarkeTech 92-5-3 Tungsten Alloy, AMS-T-21014 Class 2 Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st.. |
|||
Tensile Strength, Yield | 900 - 1100 MPa | 131000 - 160000 psi | Swaged after Sintering |
MarkeTech 93-4-3 Tungsten Alloy, AMS-T-21014 Class 2 Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st.. |
|||
Tensile Strength, Yield | 900 MPa @Strain 0.200 % |
131000 psi @Strain 0.200 % |
Typical |
Industeel CREUSABRO® 4000 High Wear Resistant Steel Description: CREUSABRO® 4000 is a high wear resistant steel, offering a 30 % extra in service life compared to a conventional 400 HB water quenched. Improved properties of CREUSABRO® 4000 resu.. |
|||
Tensile Strength, Yield | 900 MPa | 131000 psi | Typical |
Industeel CREUSABRO® 4800 Advanced Technology in Wear Steel Description: CREUSABRO® 4800(P) is a wear resistant steel offering up to 50% extra in service life compared with a 400 HB water quenched steel. CREUSABRO® 4800(P) combines several modern metal.. |
|||
Tensile Strength, Yield | 900 MPa @Strain 0.200 %, Temperature 205 °C |
131000 psi @Strain 0.200 %, Temperature 401 °F |
|
Haynes 242® alloy, cold rolled sheet, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Yield | 900 MPa @Strain 0.200 % |
131000 psi @Strain 0.200 % |
Typical |
TIMET TIMETAL® 685 (Ti-6Al-5Zr-0.5Mo-0.25Si) Titanium Alloy High-Temperature, High-Strength Creep Resistant AlloyIndustry Specifications: Germany Aerospace: 3.7154. France: T-A6ZD. UK Aerospace Specifications BS TA. 43, 44.Features: TIMETAL 685 possesses .. |
|||
Tensile Strength, Yield | 900 MPa | 131000 psi | 0° |
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass UD fabric 315 g/m2 Information provided by HexCel |
|||
Tensile Strength, Yield | 900 MPa | 131000 psi | 0° |
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass UD fabric 430 g/m2 Information provided by HexCel |
|||
Tensile Strength, Yield | 900 MPa | 131000 psi | 300% elongation; ASTM D412 |
Lubrizol Estane® 58070 Thermoplastic Polyurethane Features: Outstanding resiliency, fuel resistance and low temperature flexibility.Uses: Hose and Tube, Injection Molding, Fabric Coating and Wire/CableAvailable in Americas, Europe, Middle East, Afr.. |
|||
Tensile Strength, Yield | 900 MPa | 131000 psi | 0º |
Hexcel® HexPly® M34 75°C (167°F) Curing Epoxy Matrix, High Strength 12k Carbon Balanced Fabric 600 g/m2 Information provided by HexCel |
|||
Tensile Strength, Yield | >= 900 MPa @Strain 0.200 % |
>= 131000 psi @Strain 0.200 % |
|
CLAL-MSX NICLAFOR® 1000 TH3 Quenched/Precipitation Heat Treated, Drawn Copper Alloy Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi.. |
|||
Tensile Strength, Yield | >= 900 MPa @Strain 0.200 % |
>= 131000 psi @Strain 0.200 % |
|
CLAL-MSX NICLAFOR® 1000 TH4 Quenched/Cold Rolled/Precipitation Heat Treated, Rolled Copper Alloy Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi.. |
|||
Tensile Strength, Yield | 900 MPa @Temperature 500 °C |
131000 psi @Temperature 932 °F |
R<sub>p</sub>02. Short transverse direction. |
Assab Steels DIEVAR Hot Work Steel DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i.. |
|||
Tensile Strength, Yield | 900 MPa @Temperature 500 °C |
131000 psi @Temperature 932 °F |
R<sub>p</sub>02. austenitized 1020°C, tempered 630°C to 48 HRC. Holding time = 30 minutes. |
Assab Steels QRO 90 SUPREME Hot Work Steel QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista.. |
|||
Tensile Strength, Yield | 900 MPa @Strain 0.200 % |
131000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 20% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |
|||
Tensile Strength, Yield | 900 - 1100 MPa | 131000 - 160000 psi | |
ArcelorMittal Dual Phase 1180 Very high strength steel, Cold Rolled Steel Description: Dual Phase steels offer an outstanding combination of strength and drawability as a result of their microstructure, in which a hard martensitic or bainitic phase is dispersed in a soft .. |
|||
Tensile Strength, Yield | 900 MPa | 131000 psi | |
ThyssenKrupp SECURE MS special® Structural Steel This Material Specification applies to the high-strength thermomechanically rolled special steel SECURE MS special® (ThyssenKrupp security steel for civil use) with a hardness from 350 to 450 HBW a.. |