Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 9.65 MPa | 1400 psi | ASTM D412 |
Polymax® Maxelast® P3675 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 9.65 MPa | 1400 psi | chs 20 in/min; ASTM D412 |
Network Polymers Softflex® 7210 Black Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 9.65 MPa | 1400 psi | 510 mm/min; ASTM D412A |
PolyOne Elastamax™ EG-9190 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun.. |
|||
Tensile Strength, Yield | 9.65 MPa | 1400 psi | molding; ASTM D638 |
LyondellBasell Petrothene® NA942000 Low Density Polyethylene, Film Extrusion Grade PETROTHENE NA942 is a series of resins designed especially for heavy duty film applications, such as bags used to package fertilizer, peat moss, decorative stone and agricultural and construction ma.. |
|||
Tensile Strength, Yield | 9.65 MPa | 1400 psi | Molded; ASTM D638 |
LyondellBasell Petrothene® NA942094 Low Density Polyethylene ApplicationsPETROTHENE NA 942 is a series of resins designed especially for heavy duty film applications, such as bags used to package fertilizer, peat moss, decorative stone, and agricultural and c.. |
|||
Tensile Strength, Yield | 9.65 MPa | 1400 psi | ASTM D638 |
Global TPE-LS70A Elastomer Grade Data provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 9.65 MPa | 1400 psi | ASTM D 638 |
LyondellBasell Hifaxâ„¢ CA138A Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CA138A low modulus thermoplastic olefin (TPO) resin is designed for impact modification and injection molding applications. It is based on material produced from Basell'.. |
|||
Tensile Strength, Yield | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex APEX® 90-A472R-55-NT Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Medical Applications, Caps, Closures, Valves/Valve Parts Appearance-ClearForms-PelletsProcessing Method-.. |
|||
Tensile Strength, Yield | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex Flexalloy® 9900-55 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and .. |
|||
Tensile Strength, Yield | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2790 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2860E Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2860M Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 9.65 MPa | 1400 psi | ASTM D412 |
Teknor Apex APEX® 3210-65 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Tensile Strength, Yield | 9.65 MPa | 1400 psi | at 300%; ASTM D412 |
Lubrizol Estane® ALR E80A Thermoplastic Polyurethane Type: Estane® ALR E80A is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Information Provided by The Lubrizol Corporation |
|||
Tensile Strength, Yield | 9.65 MPa | 1400 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow DNDA-7147 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-7147 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in injection molding applications such as food containers, housewares and lids. Information provided by D.. |
|||
Tensile Strength, Yield | 9.65 MPa | 1400 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-8350 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow |
|||
Tensile Strength, Yield | 9.65 MPa | 1400 psi | ASTM D-638 |
Axiall 6570 Moldings & Extrusions Flexible PVC General purpose extrusion and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 9.65 MPa | 1400 psi | ASTM D-638 |
Axiall 8757 Moldings & Extrusions Flexible PVC Soft, general purpose, highly filled extrusion compound recommended for cove base moldings.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 9.65 MPa | 1400 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-3890MS Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedTranslucentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |
|||
Tensile Strength, Yield | 9.65 MPa | 1400 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-3890MS Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedTranslucentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |
|||
Tensile Strength, Yield | 9.65 MPa @Strain 300 % |
1400 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® IT 39-020 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerWeatherable GradeApplications:Multi-PurposeMarket:Building and ConstructionConsumer GoodsIndustrialProcessing Method:Extrusion and Moldin.. |
|||
Tensile Strength, Yield | 9.65 MPa | 1400 psi | ASTM D-638 |
Axiall 18660 Moldings & Extrusions Flexible PVC Flame retardant extrusion and molding compound recommended for 105C applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |