Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 9.114 MPa | 1322 psi | 108% Retention; Air Over Aged 1008 hrs at 100°C, Parallel |
Teknor Apex TEKRON® 4300-D88A Thermoplastic Elastomer Information provided by Teknor Apex Company |