Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 89.6 MPa | 13000 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Gravi-Tech™ GRV-NY-035-SS-GF-BLK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | ASTM D638 |
Omni Plastics OmniLon™ 6/6 PA6/6 HSL Unfilled/ Impact Modified Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Tensile Strength, Yield | 89.6 MPa @Temperature 23.9 °C |
13000 psi @Temperature 75.0 °F |
0° Direction, Dry; 325°F, 1000psi Cured; ASTM D638 |
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, Silica Reinforced Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock.. |
|||
Tensile Strength, Yield | 89.6 MPa @Temperature 23.9 °C |
13000 psi @Temperature 75.0 °F |
0° Direction, Dry; 325°F Autoclave; ASTM D638 |
Park Electrochemical Nelcote® F-554 Phenolic Prepreg, Aerospace Silica Fabric Reinforced Nelcote® F-554 is a high purity silica filled phenolic resin coated on Commercial or Aerospace grade silica fabric. F-554 is used in the manufacture of intermediate temperature ablative rocket nozz.. |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | ASTM D638 |
Polymer Resources NY66-GP2-[color]-H General Purpose Nylon 66, Nucleated, Heat Stabilized General Purpose Nylon 66, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade.. |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | ASTM D638 |
Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated General Purpose Nylon 6, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | ASTM D638 |
Polymer Resources PC/TP-GP3-G30 PC/Polyester Alloy, 30% Glass Reinforced Superior Chemical Resistance, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | ASTM D638 |
Polymer Resources TP-G15 Polybutylene Terephthalate, 15% Glass Reinforced Polybutylene Terephthalate, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N2040MHL Nylon 6 (DAM) Information provided by Ravago. |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® TR2-30GF/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | ASTM D638 |
Polymer Resources NY66-GP2 General Purpose Nylon 66, Nucleated General Purpose Nylon 66, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry.. |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | ASTM D638 |
Polymer Resources PC/ABS-G40 General Purpose PC/ABS Alloy, 40% Glass Filled PC/ABS Alloy, General Purpose, 40% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi.. |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N2040ML Nylon 6 (DAM) Information provided by Ravago. |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | ASTM D638 |
Fiberfil® J-60/30/E/HF Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, improved flow Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | ASTM D638 |
Fiberfil® J-60/30/E/M Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | ASTM D638 |
Greene Tweed Arlon® 1330 PEEK Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | ASTM D638 |
Fiberfil® J-69/20/E High performance polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | ASTM D638 |
Techmer ES Luriblend® PA6 ML2 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide Lubricant(2%)Features: Good Wear Resistance, Low Friction and LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | ISO 527 |
Westlake Plastics MediPEEK IM Polyetheretherketone for Medical Applications MediPEEK-IM is a high performance semi-crystalline thermoplastic designed for long term body contact as an implantable material. It is USP Class VI and compliant to ASTM F2026. It has excellent st.. |
|||
Tensile Strength, Yield | 89.6 - 152 MPa | 13000 - 22000 psi | 0.2% offset |
Eagle Brass 425 Tin Brass 2%, Annealed Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Tensile Strength, Yield | 89.6 - 172 MPa | 13000 - 25000 psi | 0.2% offset |
Eagle Brass 706 Copper Nickel 10%, Annealed 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | ASTM D638 |
Clariant PA123G20 Nylon 66, 20% Glass Fiber, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | ASTM D638 |
Clariant Renol PA101F/ST801 Nylon 66, Impact Modified, Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-30FG-0684 30% Glass Fiber Reinforced, Heat and UV Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-30FG-0860 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | ASTM D638 |
Techmer ES Luriblend® HTN 01410 BK Availability: North AmericaForms: PelletsAdditive: Graphite Powder Lubricant and Molybdenum Disulfide LubricantFeatures: Good Wear Resistance, Low Friction, High Heat Resistance and LubricatedAppear.. |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | Type 1 - Rigids, Break, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® NL-10GF/000 Nylon 6/12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 89.6 MPa | 13000 psi | ASTM D638 |
Polymer Resources PPX-G20 Modified PPO, 20% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |