Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 883 MPa @Strain 0.200 % |
128000 psi @Strain 0.200 % |
|
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 60% Cold Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Tensile Strength, Yield | 883 MPa @Strain 0.200 %, Temperature -73.0 °C |
128000 psi @Strain 0.200 %, Temperature -99.4 °F |
|
Carpenter Custom 450® Stainless Steel, Annealed Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Tensile Strength, Yield | 883 MPa @Strain 0.200 % |
128000 psi @Strain 0.200 % |
|
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 732°C/8hr/FC to 621°C/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |