Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 875 MPa @Strain 0.200 % |
127000 psi @Strain 0.200 % |
Precipitation Hardened. Value at room temperature |
Special Metals INCONEL® Alloy 751 A nickel-chromium alloy similar to INCONEL ALLOY X-750 but with increased aluminum content for greater precipitation hardening. INCONEL alloy 751 was designed for use as exhaust valves in internal-.. |
|||
Tensile Strength, Yield | 875 MPa @Strain 0.200 % |
127000 psi @Strain 0.200 % |
Precipitation Hardened. Value at room temperature |
Special Metals NIMONIC® Alloy 901 A nickel-iron-chromium alloy containing titanium and aluminum for precipitation hardening and molybdenum for solid-solution strengthening. The alloy has high yield strength and creep resistance at .. |