Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 870 MPa | >= 126000 psi | 60<x=80mm |
ThyssenKrupp XABO® 960 Structural Steel This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli.. |
|||
Tensile Strength, Yield | 870 MPa | 126000 psi | |
Industeel Superplast® Stainless Mold Steel SUPERPLAST® Stainless is a specially designed steel for plastic mould bases providing improved performances compared to standard grades such as 1.2085. SUPERPLAST® Stainless offers improved machi.. |