Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 834 MPa @Strain 0.200 %, Temperature -73.0 °C |
121000 psi @Strain 0.200 %, Temperature -99.4 °F |
|
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 20% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |
|||
Tensile Strength, Yield | 834 MPa | 121000 psi | |
HP Alloys HPA COBALT Alloy 6BH, Wear Resistant, (Co-Cr-W) (UNS R30016) Cobalt 6BH is the same composition of Cobalt 6B, except the material is hot rolled and then age hardened. The direct age-hardening after hot rolling provides the maximum hardness and wear resistance.. |