Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 8.96 MPa | 1300 psi | at 2% Offset; ASTM D638 |
ExxonMobil LD 509.48 Compounding Resin
(discontinued **) LD 509.48 is a high melt index homopolymer resin designed to provide good processability in compounding applications.Information provided by ExxonMobil Chemical |
|||
Tensile Strength, Yield | 8.96 MPa | 1300 psi | ASTM D638 |
M. Holland Company LD300 LDPE
(discontinued **) Features: High ESCR (Stress Crack Resist.), Good Processability, Low Temp. StrengthUses: Closures, Electrical Parts, Household GoodsApprovals: FDA 21 CFR 177.1520(c) 2.2Processing Method: Injection .. |
|||
Tensile Strength, Yield | 8.96 MPa @Temperature 23.0 °C |
1300 psi @Temperature 73.4 °F |
ASTM D638 |
Ineos T00G-00 Polypropylene Impact Copolymer This is a fractional MFR polypropylene impact copolymer designed for the roofing membrane market. Its blend of impact resistance and flexural modulus is designed to provide an excellent balance bet.. |
|||
Tensile Strength, Yield | 8.96 MPa | 1300 psi | ASTM D638 |
LyondellBasell Petrothene® NA831000 Low Density Polyethylene ApplicationsPETROTHENE NA831-000 resin exhibits high stress crack resistance and low temperature brittleness. Typical applications include housewares, containers and industrial parts. Regulatory St.. |
|||
Tensile Strength, Yield | 8.96 MPa | 1300 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 7204 LC TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Tensile Strength, Yield | 8.96 MPa | 1300 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 7802 TPE Blk Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tensile Strength, Yield | >= 8.96 MPa | >= 1300 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7148 Fluorocarbon-Elastomer FKM specially for oil & gas service; ED resistantInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 8.96 MPa | 1300 psi | AVG Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 7267 Ethylene-Propylene Rubber EPDM for high temperature steam service. Also available as a Y267-Type (7267L).Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex APEX® 1700-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose, Low Gloss Uses-Appliance Components, Footwear, FurnitureForms-PelletsProcessing Met.. |
|||
Tensile Strength, Yield | 8.96 MPa | 1300 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3301-80 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Tensile Strength, Yield | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex APEX® 3310-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Tensile Strength, Yield | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex APEX® 3311-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Tensile Strength, Yield | 8.96 MPa | 1300 psi | 100%; ASTM D412 |
Teknor Apex Flexalloy® 3501-75-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |
|||
Tensile Strength, Yield | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2850M Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | >= 8.96 MPa | >= 1300 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7182B Fluorocarbon-Elastomer Formulated AFLAS® high-temperature, high-pressure "sour" oil & gas service. ED resistant. Excellent acid and base resistance.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex TEKBOND® MP 1723 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex UNIPRENE® 7010-87 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 8.96 MPa @Strain 300 % |
1300 psi @Strain 300 % |
ASTM D412 |
Clariant OMAN698583 Thermoplastic Polyurethane, Halogen Free, Flame Retardant Aromatic Polyether BasedData provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 8.96 MPa | 1300 psi | ASTM D-638 |
Axiall 53061A Moldings & Extrusions Flexible PVC General purpose injection molding and extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 8.96 MPa | 1300 psi | ASTM D-638 |
Axiall 7540 Moldings & Extrusions Flexible PVC A high quality clear outdoor grade PVC molding and extrusion compound formulated for good UV light resistance and excellent low temperature properties.Information provided by Georgia GulfGeorgia Gul.. |
|||
Tensile Strength, Yield | 8.96 MPa | 1300 psi | ASTM D638 |
Multibase Multi-Flam™ 0803 LDPE NH Polyethylene Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Injection MoldingExtrusionCoextrusionUses:TubingPipingInformation provided by Multibase |
|||
Tensile Strength, Yield | 8.96 MPa | 1300 psi | ASTM D638 |
Aaron Industries AVPE LD 300-1 MELT 20 Virgin Polyethylene A natural, high flow Low Density Polyethylene resin, specifically designed for high speed injection molding applications. |
|||
Tensile Strength, Yield | 8.96 MPa | 1300 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-3870E Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:ExtrusionPolyOne First ChoiceDisclaimer: A ther.. |
|||
Tensile Strength, Yield | 8.96 MPa | 1300 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 8103 E Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection MoldingExtrusions Information provided by Multibase |
|||
Tensile Strength, Yield | 8.96 - 35.2 MPa | 1300 - 5110 psi | Average value: 25.1 MPa Grade Count:200 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |
|||
Tensile Strength, Yield | 8.96 - 110 MPa | 1300 - 16000 psi | Average value: 26.4 MPa Grade Count:712 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |