Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 8.1579 MPa | 1183.2 psi | Air at 302°F, 168 hr; ASTM D573 |
ExxonMobil Santoprene® 273-50 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Tensile Strength, Yield | 8.1579 MPa | 1183.2 psi | Air at 302°F, 168 hr; ASTM D573 |
ExxonMobil Santoprene® 203-50 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |