Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Network Polymers Nylon 0304NL Description: Natural NylonInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Ravago Manufacturing Americas Hylex® P1025G10 HB Polycarbonate, 10% Glass Reinforced Information provided by Ravago. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N2000HL Nylon 6 (DAM) Information provided by Ravago. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ 80520 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Ensinger ENSITEP® PET Polyethylene Terephthalate - Extruded Products
(discontinued **) ENSITEP is an unreinforced, semi-crystalline thermoplastic polyester derived from polyethylene terephthalate. Its excellent wear resistance, low coefficient of friction, high flexural modulus, and .. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | Type 1 - Rigids, Break, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AS-30GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Lord Adhesives Thermosetâ„¢ EP-809 Ignition Coil Impregnating and Encapsulation Epoxy Lord EP-809 is a long working life, heat curing, two component epoxy formulation. It was designed especially for potting high voltage automotive ignition coils. The combination of low viscosity, exc.. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | .01% permanent set |
Meehanite GE-30 Flake Graphite Cast Iron Type GE-30 combines improved strength and solidity with higher machining feeds and speeds than ordinary gray iron.General Meehanite information - Meehanite metal is first melted to a definite degree.. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Techmer ES Electrablend® PA6/PC Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Conductive Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Spartech PP5430 Glass Fiber Reinforced Homopolymer Provides the maximum strength and heat resistance among polypropylene compounds. Physical properties can approach those of more expensive engineering resins.Information provided by Spartech |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF30 L 30% Milled Glass Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Glass Fiber, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Techmer ES HiFill® PA6 HS L BK Heat Stabilized Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: BlackTPCI# 7190102Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Techmer ES HiFill® PA6 HS L Colors Heat Stabilized Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: Colors AvailableTPCI# 10014102Information provided by TP Composite.. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Techmer ES HiFill® PA6 NAT Availability: North AmericaForms: PelletsFeatures: Low ViscosityTPCI# 1026102Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF10 TL10 BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: Heat Stabilizer and PTFE Lubricant(10%)Features: Lubricated and Heat Stabiliz.. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF12 TL20 12% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 12% Filler by Weight Additive: Heat Stabilizer and PTFE Lubricant(20%)Features: Lubricated and Heat Stabiliz.. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Techmer ES HiFill® PET 0268 B1 Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Techmer ES Luriblend® PA6 E ML2 MB Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Techmer ES Luriblend® POM CO GF10 TX15 BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Copolymer, Good Wear Resistance and Low FrictionApp.. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Techmer ES Electrablend® PA6 C BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Chase Plastics CP Pryme® NN100M2 (Dry) Nylon 66, Lubricated Features: Good chemical resistanceFast cycleDurableLubricatedSolvent resistantInjection moldingForm: PelletsInformation provided by Chase Plastics. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Clariant Renol PA211 Nylon 6, General Purpose Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Entec Hylex® P1025G10NHFR Polycarbonate, 10% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-43FG-0410 43% Glass Fiber Reinforced, Heat and UV Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Asahi Kasei Thermofil N-40MF-1600 40% Mineral Filled, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-40FM-2371 40% Glass Fiber/Mica Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
LNP Konduit® ITF-212-11 Polyamide 6/12 Copolymer
(discontinued **) Features: Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades ar.. |
|||
Tensile Strength, Yield | 79.3 MPa | 11500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AT-25GF-10MN/000 BLASCK Acetal-Copolymer, Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |