Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 78.6 MPa | 11400 psi | ASTM D 638 |
LyondellBasell Hostacomâ„¢ BJ23A Polypropylene Copolymer Description: Hostacomâ„¢ BJ23A is a polypropylene copolymer that is used for appliance componentsFeatures: Good StiffnessGood FlowChemically CoupledGood Impact ResistanceInformation provided by B.. |
|||
Tensile Strength, Yield | 78.6 MPa | 11400 psi | ASTM 638 |
PlastxWorld CEVIAN® VGR20 20% GF ABS Glass fiber reinforced ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |