Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 758 MPa @Strain 0.200 % |
>= 110000 psi @Strain 0.200 % |
|
Materion ToughMet® T3 AT110 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Tensile Strength, Yield | 758 MPa @Strain 0.200 % |
110000 psi @Strain 0.200 % |
|
Haynes Hastelloy® C-22® alloy, 10% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Yield | 758 MPa | 110000 psi | |
HP Alloys Alloy 718, 10% Cold Worked 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Tensile Strength, Yield | 758 - 965 MPa @Strain 0.200 % |
110000 - 140000 psi @Strain 0.200 % |
|
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed and Aged Rod and Bar specifically. Other property values are typic.. |
|||
Tensile Strength, Yield | 758 MPa | 110000 psi | Cold Worked |
Special Metals INCOLOY® alloy 028 Austenitic Stainless Steel INCOLOY® alloy 028 (UNS N08028/W. Nr. 1.4563) is a highly alloyed austenitic stainless steel offering resistance to a variety of corrosive media. By virtue of its contents of chromium and molybd.. |
|||
Tensile Strength, Yield | 758 - 896 MPa @Strain 0.200 % |
110000 - 130000 psi @Strain 0.200 % |
Heat Treatment (Condition T HRc 26-32) |
Schmolz + Bickenbach 416 Stainless Steel Bar Description: Ugitech’s 416 is free machining martensitic grade. The unique production process—developed exclusively by Ugitech—results in a product that delivers superior productivity.. |
|||
Tensile Strength, Yield | 758 MPa @Strain 0.200 % |
110000 psi @Strain 0.200 % |
|
Schmolz + Bickenbach MoldMAX LH® Low Hard - Copper Alloy Description: Brush Wellman’s MoldMAX LH® (Low Hard) is a premium copper mold alloy that provides hardness and strength comparable with standard AISI P-20 tool steel and a thermal conductivit.. |
|||
Tensile Strength, Yield | 758 MPa @Strain 0.200 % |
110000 psi @Strain 0.200 % |
Typical |
TIMET TIMETAL® 5111 Titanium Alloy (Ti-5Al-1Sn-1Zr-1V-0.8Mo; ASTM Grade 32) High Toughness, Heavy Section Weldable AlloyFeatures: A near alpha alloy with excellent weldability, seawater stress corrosion cracking resistance and high dynamic toughness. It is ideally suited f.. |
|||
Tensile Strength, Yield | >= 758 MPa | >= 110000 psi | 0.2% Offset |
Eagle Brass 301 Austenitic Stainless Steel, 1/2 Hardened Type 301 is a chromium-nickel stainless steel that provides high strength and good ductility with chromium and nickel contents lowered to increase the work hardening range. This permits higher tens.. |
|||
Tensile Strength, Yield | >= 758 MPa | >= 110000 psi | 0.2% Offset |
Eagle Brass 302 Austenitic Stainless Steel, 1/2 Hardened Types 302 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Tensile Strength, Yield | >= 758 MPa | >= 110000 psi | 0.2% Offset |
Eagle Brass 304 Austenitic Stainless Steel, 1/2 Hardened Types 304 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Tensile Strength, Yield | >= 758 MPa | >= 110000 psi | 0.2% Offset |
Eagle Brass 305 Austenitic Stainless Steel, 1/2 Hardened Type 305 is a chromium nickel stainless steel that can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is nonmagnetic under most conditions. .. |
|||
Tensile Strength, Yield | >= 758 MPa | >= 110000 psi | 0.2% Offset |
Eagle Brass 316 Austenitic Stainless Steel, 1/2 Hardened The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 .. |
|||
Tensile Strength, Yield | >= 758 MPa | >= 110000 psi | 0.2% Offset |
Eagle Brass 316L Austenitic Stainless Steel, 1/2 Hardened Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a.. |
|||
Tensile Strength, Yield | >= 758 MPa | >= 110000 psi | 0.2% Offset |
Eagle Brass 304L Austenitic Stainless Steel, 1/2 Hardened Type 304L is a very common variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled. Lower carbon 304L minimizes chromium ca.. |
|||
Tensile Strength, Yield | 758 - 827 MPa @Strain 0.200 % |
110000 - 120000 psi @Strain 0.200 % |
|
Ametek AM 388™ Alloy (UNS C72650) TX00 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Tensile Strength, Yield | 758 MPa @Strain 0.200 %, Temperature 538 °C |
110000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Carpenter Custom 455® Stainless Steel, Condition H950 (Age Hardened 510°C) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
Tensile Strength, Yield | >= 758 MPa @Strain 0.200 % |
>= 110000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Stainless Steel Type 301, 1/2 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Tensile Strength, Yield | 758 MPa | 110000 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 30% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Tensile Strength, Yield | 758 MPa @Strain 0.200 % |
110000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 538°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Tensile Strength, Yield | >= 758 MPa @Strain 0.200 % |
>= 110000 psi @Strain 0.200 % |
|
Materion ToughMet® T3 AT110 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin.. |