Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 752 MPa @Temperature 23.9 °C |
109000 psi @Temperature 75.0 °F |
0° Direction, Dry; Oven Cure 275°F, 90 min; ASTM D638 |
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 3K 2x2 Twill Carbon Reinforced Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra.. |
|||
Tensile Strength, Yield | 752 MPa @Strain 0.200 %, Temperature 199 °C |
109000 psi @Strain 0.200 %, Temperature 390 °F |
hardened to 310 HB |
Bohler-Uddeholm HOLDER Pre-hardened Holder Tool Steel Chromium-molybdenum alloyed steelA pre-hardened steel with very good machinability supplied at ~300 HB for clamping and holding plates and blocks.Holder is characterized by: Excellent machinability.. |