Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 723 MPa | 105000 psi | |
CMW® THERMKON® 62 Tungsten Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Tensile Strength, Yield | 723 - 861 MPa | 105000 - 125000 psi | |
Ametek AM 388™ Alloy (UNS C72650) TM06 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |