Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 7.3968 MPa @Treatment Temp. 125 °C, Time 252000 sec |
1072.8 psi @Treatment Temp. 257 °F, Time 70.0 hour |
Heat Aging; ASTM D573 |
Vicone High Performance Rubber VicoSil™ 909E-BK High Performance Silicone Rubber Information provided by Vicone |