Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 69.6 MPa | 10100 psi | chs 2 in/min; ASTM D638 |
Network Polymers SAN 290 Light Blue Tint Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | >= 69.6 MPa @Strain 0.200 %, Temperature 249 °C |
>= 10100 psi @Strain 0.200 %, Temperature 480 °F |
|
H.C. Starck NRC® Tantalum (UNS R05200) Applications: High strength and excellent corrosion resistance make tantalum ideal for use in the manufacture and repair of chemical process equipment and heat exchangers. Other uses are rupture di.. |
|||
Tensile Strength, Yield | 69.6 MPa | 10100 psi | ASTM D638 |
Techmer ES Electrablend® PC 04006 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite.. |
|||
Tensile Strength, Yield | 69.6 MPa | 10100 psi | ASTM D638 |
Solvay Specialty Polymers Radel® R-5100 Polyphenylsulfone (PPSU), Filled Radel® R-5100 is an opaque, general purpose polyphenylsulfone (PPSU) for injection molding, that offers exceptional hydrolytic stability, and toughness superior to other commercially-available, h.. |
|||
Tensile Strength, Yield | 69.6 MPa | 10100 psi | ASTM D638 |
Samyang Trirex® 3025L1 Polycarbonate, Lens Grade TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Tensile Strength, Yield | 69.6 MPa | 10100 psi | ASTM D638 |
Techmer ES HiFill FR® PA6 FR 544 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedRoHS Compliance: RoHS CompliantInformation provided by TP Com.. |
|||
Tensile Strength, Yield | 69.6 MPa | 10100 psi | ASTM D638 |
Samyang Trirex® 3025A Polycarbonate TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Tensile Strength, Yield | 69.6 MPa | 10100 psi | ASTM D638 |
Westlake Plastics Radel® R 4400 Polyphenylsulfone For Medical Applications Medical grade Radel R4400 resin offers exceptional hydrolytic stability, toughness, heat deflection temperature and resistance to stress cracking. This polymer also has excellent thermal stability,.. |
|||
Tensile Strength, Yield | 69.6 MPa | 10100 psi | ASTM D638 |
Westlake Plastics Radel® R 5500 Polyphenylsulfone Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness, and good environmental stress c.. |
|||
Tensile Strength, Yield | 69.6 MPa | 10100 psi | ASTM D638 |
Westlake Plastics Radel® R 5500 Polyphenylsulfone For Medical Applications Medical grade Radel R5500 resin offers exceptional hydrolytic stability, toughness, heat deflection temperature and resistance to stress cracking. This polymer also has excellent thermal stability,.. |
|||
Tensile Strength, Yield | 69.6 MPa | 10100 psi | ASTM D638 |
Westlake Plastics Radel® R Polyphenylsulfone Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness and good environmental stress cr.. |
|||
Tensile Strength, Yield | 69.6 MPa | 10100 psi | ASTM D638 |
Ensinger TECASON™ P MT Polyphenylsulfone (PPSU) TECASON™ P MT is a polyphenylsulfone suited primarily to applications in the medical industry. It has improved performance in terms of temperature, impact strength and chemical resistance, as well.. |
|||
Tensile Strength, Yield | 69.6 MPa | 10100 psi | ASTM D638 |
Ensinger TECASON™ P Polyphenylsulfone (PPSU) TECASON™ P is a polyphenylsulfone that exhibits excellent temperature, impact and chemical resistance properties. |
|||
Tensile Strength, Yield | 69.6 MPa @Temperature 22.8 °C |
10100 psi @Temperature 73.0 °F |
ASTM D638 |
Ensinger RADEL® R-5500 Polyphenylsulfone (PPSU) RADEL® R is a Polyphenysulfone produced by Solvay Advanced Polymers. RADEL® R is in the same performance category as products like Polysulfone and ULTEM® (PEI). RADEL® R has increased performa.. |