Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 638 MPa @Strain 0.200 % |
92500 psi @Strain 0.200 % |
|
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 15.9 mm thick bar Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Tensile Strength, Yield | 638 MPa @Strain 0.200 % |
92500 psi @Strain 0.200 % |
|
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 15.9 mm thick plate, aged 3 hours at 816°C Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |