Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 60.7 MPa | 8800 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ PC-000/10T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® AT-1000 Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Strength, Yield | 60.7 - 68.0 MPa | 8800 - 9860 psi | Average value: 64.6 MPa Grade Count:4 |
Overview of materials for Acrylic, High Flow, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, High Flow, Molded". Each property range of values reported is minimum and maximum values of app.. |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Fiberfil® J-62/30/E8 Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Techmer ES HiFill® PA6 L UV (Conditioned) Availability: North AmericaForms: PelletsAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Techmer ES Luriblend® PA6/12 05007 Nylon 612 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Techmer ES Plastiblend® POM CO UV BK Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: CopolymerAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM Data |
Styron CALIBRE™ 701 15 Polycarbonate, General Purpose CALIBRE® 701 series polycarbonate resins are a general purpose, transparent, ignition resistant grades equipped with a mold release package. The CALIBRE 701 series resins exhibit a high heat resi.. |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Techmer ES HiFill® HDPE LGF50 12 mm 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Styron EMERGEâ„¢ 4600-10 Polycarbonate EMERGEâ„¢ PC 4600-10 advanced resin is formulated to supply both clarity and enhanced ignition resistance while maintaining excellent physical properties. Applications: Information Technology E.. |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Sumitomo Chemical Sumipex® LG35 Acrylic Resin, High Flow Product CharacteristicsHigh FlowImproved Cycle TimeInformation provided by Calsak Corporation |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Westlake Plastics Pomalux® Acetal Copolymer Pomalux is a high performance acetal copolymer that has excellent mechanical, electrical, and wear properties. It is engineered to provide outstanding dimensional stability, even when machining par.. |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Clariant Renol PCSP0006 Polycarbonate, Laser Markable Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Ensinger Tecaform™ Acetal Copolymer - Extruded Products (POM) Tecaform™ is a semi-crystalline thermoplastic offering high strength, stiffness and toughness. It is resistant to hot water, hydrocarbons and solvents, and it posses good bearing and wear properti.. |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Ensinger Tecast Vekton™ 6PAG Graphite-Filled Cast Nylon 6 (PA6) Tecast® 6PAG is a graphite powder-filled with properties similar to MoS2-filled but better suited to wet applications.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a vari.. |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Ensinger Tecast Vekton™ 6PAM MoS2-Filled Cast Nylon 6 (PA6) Tecast® 6PAM is a molybdenum disulfide-filled cast nylon 6 used for general bearings and wear applications and for its superior strength and hardness.General Tecast® Cast Nylon Information: Tecast.. |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Asahi Kasei Thermofil D-10FG-1101 10% Glass Fiber Reinforced, ABS Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 60.7 MPa | 8800 psi | ASTM D638 |
Fiberfil® J-62/30/E Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |