Mechanical Properties Metric English Comments
Tensile Strength, Yield 6.30 MPa
914 psi
ASTM D412
Polymax® Maxelast® S4670 TPE, PS Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesSporting GoodsInformation from Alliance Polymers & Services, Distributor of Nantong ..
Tensile Strength, Yield 6.30 MPa
914 psi
-10% change after 70 hours @ 204°C; ASTM D412
Precision Polymer Engineering F60A Fluorosilicone Rubber
Blue Fluorosilicone, 56-65 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification Mil-R-25988B, Class 1, Grade 60...
Tensile Strength, Yield 6.30 - 11.7 MPa
914 - 1700 psi
±30% change after 70 hours @ 100°C; ASTM D412
Precision Polymer Engineering J70M Butyl Rubber
Bromobutyl Rubber, 65-75 IRHD. Brominated isobutylene-isoprene copolymer. To meet BS3227 Grade 70 and ASTM D2000 line call-out MBA708, F17.Applications: Bromobutyl is resistant to the same fluids a..
Tensile Strength, Yield 6.30 MPa
914 psi
-30% change after 70 hours @ 150°C; ASTM D412
Precision Polymer Engineering P60B Polyacrylate Rubber
Polyacrylic or Polyacrylate Rubber, 55-65 °IRHD. Copolymer of ethyl acrylate and vinyl ether. ASTM & ISO designation = ACM.Applications: Extensively used in automotive transmission systems. Superi..
Tensile Strength, Yield 6.30 MPa
914 psi
-30% change after 70 hours @ 150°C; ASTM D412
Precision Polymer Engineering P90B Polyacrylate Rubber
Polyacrylic or Polyacrylate Rubber, 85-95 °IRHD. Copolymer of ethyl acrylate and vinyl ether. ASTM & ISO designation = ACM.Applications: Extensively used in automotive transmission systems. Superi..
Tensile Strength, Yield 6.30 MPa
914 psi
-30% change after 70 hours @ 200°C; ASTM D412
Precision Polymer Engineering S70B Silicone Rubber
Black Silicone Rubber, 66-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Excellent heat resistance and ..
Tensile Strength, Yield 6.30 MPa

@Strain 100 %
914 psi

@Strain 100 %
ISO 527-1/-2
Covestro Desmopan® W DP 85786A Polyurethane
Grade for calanderingno yellowing under the action of UV lightgood low-temperature flexibilityhigh rebound resilienceimproved microbial resistanceImproved hydrolysis resistanceApplicationTextile coa..
Tensile Strength, Yield 6.30 MPa
914 psi
508 mm/min; ASTM D638
Dow Engage® 8450 Polyolefin Elastomer
Description: Engage® 8450 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It has excellent compatibility with other p..
Tensile Strength, Yield 6.30 MPa
914 psi
508 mm/min; ASTM D638
Dow Engage® 8402 Polyolefin Elastomer
Description: Engage® 8402 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in durable, flexible injection molded industrial and consumer goods. Engage® 8402 pr..
Copyright © lookpolymers.com All Rights Reserved