Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 580 MPa @Strain 0.200 % |
84100 psi @Strain 0.200 % |
|
Hogen HM1150 Tungsten-Based Metal Mil Spec T-21014D Class 2; AMS T-21014 Class 2; ASTM B-777-99 Class 2. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE.. |
|||
Tensile Strength, Yield | 580 MPa @Strain 0.200 % |
84100 psi @Strain 0.200 % |
|
Mi-Tech Metals HD17.5 Tungsten-Based Metal Mil Spec T-21014D Class 2; AMS T-21014 Class 2; ASTM B-777-99 Class 2; ASTM B-777-07 Class 2. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal con.. |
|||
Tensile Strength, Yield | >= 580 MPa @Strain 1.00 % |
>= 84100 psi @Strain 1.00 % |
|
Industeel SOLEIL C5 13% Cr 4 Ni Martensitic Stainless Steel with Improved Toughness Description: Soleil C5 is a 13% Cr 4 Ni 0.5 Mo martensitic stainless steel. Its nickel content, associated with low carbon ensures better weldability, ductility, impact resistance and fatigue resist.. |
|||
Tensile Strength, Yield | 580 MPa @Strain 0.200 % |
84100 psi @Strain 0.200 % |
|
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Tensile Strength, Yield | 580 MPa @Strain 0.200 % |
84100 psi @Strain 0.200 % |
|
Bisalloy Steels BisPlate 60 Thickness 5 - Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness.Applications: Storage Tanks, High Rise Buildings, Lifting Equipment.. |
|||
Tensile Strength, Yield | 580 MPa @Strain 0.200 % |
84100 psi @Strain 0.200 % |
|
Bisalloy Steels BisPlate 60 Thickness >80-100 mm Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness.Applications: Storage Tanks, High Rise Buildings, Lifting Equipment.. |
|||
Tensile Strength, Yield | 580 MPa @Strain 0.200 % |
84100 psi @Strain 0.200 % |
|
Bisalloy Steels BisPlate 60 Thickness 16-80 mm Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness.Applications: Storage Tanks, High Rise Buildings, Lifting Equipment.. |
|||
Tensile Strength, Yield | 580 MPa | 84100 psi | |
Latrobe Nitralloy® 135 Modified VAC-ARC, 3 to 5 in Premium Nitriding Steel NITRALLOY 135 MODIFIED VAC-ARC steel is a low alloy nitriding grade with moderate hardenability. It has been designed to provide a high case hardness and to maintain its core strength during the nit.. |