Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 55.2 MPa | 8000 psi | chs 2 in/min; ASTM D638 |
Network Polymers NPP 808 C2WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Polymer Resources PC-FR3A-D Polycarbonate, Flame Retardant, High Flow Polycarbonate, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Polymer Resources PC-GP1-10TFE Polycarbonate, General Purpose, Wear Resistant, Low Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 55.2 MPa @Thickness 3.17 mm |
8010 psi @Thickness 0.125 in |
ASTM D638 |
PTS PCA-1012 High Impact Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N2000STHL Nylon 6 (DAM) Information provided by Ravago. |
|||
Tensile Strength, Yield | 55.2 MPa @Thickness 3.17 mm |
8010 psi @Thickness 0.125 in |
ASTM D638 |
PTS Tristar® PC-10R-(IM) 10 MFI Impact Modified Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 55.2 MPa | 8010 psi | 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® X TR2-30TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Tensile Strength, Yield | 55.2 - 82.7 MPa | 8000 - 12000 psi | ASTM D638 |
Alcoa KAMA 2200 Prime Graphic Arts OPS
(discontinued **) CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti.. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Polymer Resources PC-FR1-D-[color]-3 Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
M. Holland Company PCAB250 Acrylonitrile Butadiene Styrene + PC High heat resistanceHigh impact resistanceLow temperature impact resistanceApplications: Automotive |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
MRC Polymers NAXELLâ„¢ PC429HHI Polycarbonate, Impact Modified, High MFR, EZ Flow Good Property RetentionHeat and Dimensional StabilityHigh Melt Impact ModifiedMFR can be modified between 10 to 26 g/10minsCan be UV stabilizedGenerally for natural, colorable and can go blackIntern.. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Techmer ES Elastoblend® PA6 IM 7040 MB Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier, Nucleating Agent and LubricantFeatures: Heat Stabilized, Impact Modified, Nucleated and LubricatedInformation pro.. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Techmer ES HiFill® HDPE GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Techmer ES HiFill® PBT 613 Availability: North AmericaForms: PelletsFeatures: Good Flow and Good ProcessabilityAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Techmer ES Plastiblend® PA6/6,6 IM HS L Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedProcessing Method: Injection Mold.. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Techmer ES Statiblend® POM CO AS Availability: North AmericaForms: PelletsAdditive: AntistaticFeature: Antistatic and ConductiveTPCI# 60000114Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Techmer ES HiFill FR® PC FR HS GY154 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and UV StabilizerFeatures: Flame Retardant and Heat StabilizedAppearance: GreyInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Chase Plastics CP Pryme® AC300 Acetal Copolymer, Recycled Content Features: Recycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Tensile Strength, Yield | 55.2 - 131 MPa | 8000 - 19000 psi | 0.2% offset |
Eagle Brass 230 Red Brass, Annealed CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ASA TWP 121 Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Clariant Renol BR7008 Polycarbonate/Polyester Alloy Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Clariant Renol PBT1100S Polybutylene Terephthalate, Silicone Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Clariant Renol PCSP0016BL-201 Polycarbonate/Polyester Alloy Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Ensinger Tecamid® 6/12 Nylon (PA612) Type 6/12 has lower moisture absorption rates than nylon 6/6, hence superior dimensional stability.Information provided by Ensinger, Inc. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Asahi Kasei Thermylene® P1-35FM-1374H 35% Glass/Fiber Reinforced Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 55.2 MPa | 8010 psi | ASTM D412 |
C.O.I.M. LARIPUR® LPR8025 Special Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
Techmer ES Luriblend® POM CO SL2 MB Acetal Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and CopolymerTPCI# 9809114Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
PlastxWorld Veroplas PA2002MI Nylon 6 general purpose, unfilled, medium impact modified injection molding gradeInformation provided by PlastxWorld Inc. |