Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 55.0 MPa | 7980 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS (Asia Pacific) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce.. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Europe-Africa-Middle East) 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Asia Pacific) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel.. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | ISO 527-1/-2 |
Mitsubishi Xantar® MX 1001 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | ISO 527-1/-2 |
Mitsubishi Xantar® MX 1002 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 325 PBT (Europe-Africa-Middle East) VALOX 325 is a general purpose, unreinforced PBT injection moulding resin. Applications: sprinklers and nozzles, pumps, doorhandles, tank covers, pens and pencils. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Europe-Africa-Middle East) LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Asia Pacific) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Europe-Africa-Middle East) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Xylex X8300HP PC+POLYESTER (Asia Pacific) Transparent, US Food Contact compliant, chemically resistant.
This grade will no longer be supported with biocompatibility information and should not be used for medical applications which require b.. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xylex X8419 PC+POLYESTER Low-medium flow, suitable for blow molding, injection molding, extrusion.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Asia Pacific) design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Asia Pacific) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® FXV310SK PBT VALOX FXV310SK is an unreinforced PBT injection moulding Visualfx* resin with high flow characteristics and containing a metal sparkle. Applications: automotive bezels and appliances. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | ISO 527-2 |
Tisan TISESTER® UNR Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 1080 Glass Fiber-Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1080 is a 20% fiber-reinforced homopolymer polypropylene with excellent strength and heat resistance. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 50 mm/min; ISO 527 |
CP-Polymer-Technik Wellamid® 6600 HW Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 50 mm/min; ISO 527 |
CP-Polymer-Technik Wellamid® 6600/58 HWCP Nylon 66, Impact Modified Until -40°C, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | ISO 527-1/-2 |
DSM Stanyl® TW441 (COND) Nylon 46 High Viscosity, Heat Stabilized, Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized High Viscosity Polyamide 66 Zytel E51HSB NC010 is a high molecular weight heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by .. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 5 mm/min; ISO 527 |
Eurostar Staramide PK005EI2 PA6, Mineral Fiber Filled, Impact Modified Injection Molded Staramide PK005EI2 is an Impact Modified Mineral Filled Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | ISO 527 |
Azoty Tarnow™ TARNOFORM 300 SI POM Tribological modified grade with silicon, for better sliding properties in plastic-plastic contact.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | |
BASF Gusspolyamid® Nylon 6 (At 50% RH) Processed by anionic polymerization of caprolactam in the presence of a catalyst and activator. Uses include semi-finished products and containers (e.g. heating oil tanks).Data was collected by ISO.. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® 21SPC Nylon 66, Conditioned Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering .. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PX1005X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, Conditioned Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou.. |