Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 53.0 MPa | 7690 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS (Europe-Africa-Middle East) High flow PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer (Asia Pacific) 6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S.. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® ML7666 PC (Asia Pacific) Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque onlyThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | ISO 527 |
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Asia Pacific) LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | ISO 527 |
SABIC Innovative Plastics LNP FARADEX WX94736 PBT LNP* Faradex* WX94736 is a compound based on Polybutylene Terephalate resin containing Stainless Steel. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL002P PC (Asia Pacific) LNP LUBRICOMP* DL002P is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Exceptional Processing. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DL0039E PC (Europe-Africa-Middle East) LNP* LUBRICOMP* DL0039E is a compound based on Polycarbonate resin containing PTFE, Flame retardant. Added features include: Easy Molding, Internally Lubricated, Flame retardant. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD4271 PC Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility.. |
|||
Tensile Strength, Yield | 53.0 MPa @Thickness 3.20 mm |
7680 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical HT700 ABS, High Stiffness Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Strength, Yield | 53.0 MPa @Thickness 3.20 mm |
7680 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical XG568 MABS, Anti-Scratch, High Gloss Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KP003AXZ Acetal Homopoly (Asia Pacific) LNP* Lubricomp* KP003AXZ is a compound based on Acetal Homopolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | ISO 527 type 1 A |
Solvay TECHNYL® A 50H1 PA66, Conditioned Description: Flame retardant polyamide 66, unreinforced, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This phospho.. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR5210R PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_WR5210R compound is a wear resistant, 7% PTFE filled material. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP NL001 PC+ABS LNP LUBRICOMP* NL001 is a compound b ased on PC+ABS resin containing 5% PTFE. Added features include: Wear Resistant, Suitable for Thin Wall Applications. |
|||
Tensile Strength, Yield | 53.0 - 57.0 MPa @Thickness 2.00 mm |
7690 - 8270 psi @Thickness 0.0787 in |
50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF) Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: Batteries; Membran.. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Asia Pacific) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Asia Pacific) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Europe-Africa-Middle East) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PVX0800 PPE NORYL* PVX0800 resin is a high flow, V0 = 1.5 mm grade, suitable for a variety of electronics applications. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer LNP* STAT-KON* KD000 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | 2 in/min; ASTM Test |
Styrolution Terblend® N NG-02 8% Glass Filled ABS/PA6 (Dry) Terblend N NG-02 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, high impact strength and good surface appearance.Information provided by STYROLUTION, which is a join.. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | ASTM D638 |
Wanshijie PETG Sheet PETG is also named GPET. It is made of a kind of non-crystalline PET resin sourced from cyclohexanediol modification. PETG differs greatly from PET and PCT. PETG is a kind of non-crystalline copolym.. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | ASTM D638 |
Eastman Aspira EN177 Copolyester Resin for Extrusion Blow Molding Applications:Beverage packagingConsumer packagingFood packagingPersonal care packagingKey Attributes:BPA-freeCompatible with high-output manufacturing platformsExcellent clarityHigh gloss appearance.. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | chs 5 mm/min; ASTM D638 |
Diamond Polymers ABSPC 7330-1801H ABS/PC Injection Molding Grade Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 53.0 MPa @Temperature 80.0 °C |
7690 psi @Temperature 176 °F |
ISO Data |
BASF Ultramid® B3ZG3 15% Glass Filled PA6 (Dry) Ultramid B3ZG3 is an impact-modified, 15% glass fiber reinforced injection molding PA6 grade. |
|||
Tensile Strength, Yield | 53.0 - 57.0 MPa | 7690 - 8270 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer
(discontinued **) Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS (Asia Pacific) Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only. |
|||
Tensile Strength, Yield | 53.0 MPa | 7690 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL0039EF PC LNP* Lubricomp* DL-0039EF is a compound based on Polycarbonate resin containing 15% PTFE. Characteristics of this grade include: Flame Retardant and Internally Lubricated. |