Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 520 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 520 MPa
>= 75400 psi
H.C. Starck HPM 1700 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Tensile Strength, Yield >= 520 MPa
>= 75400 psi
H.C. Starck HPM 1701 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Tensile Strength, Yield >= 520 MPa
>= 75400 psi
H.C. Starck HPM 1705 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Tensile Strength, Yield >= 520 MPa
>= 75400 psi
H.C. Starck HPM 1710 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Tensile Strength, Yield >= 520 MPa
>= 75400 psi
H.C. Starck HPM 1750 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Tensile Strength, Yield >= 520 MPa
>= 75400 psi
H.C. Starck HPM 1760 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Tensile Strength, Yield >= 520 MPa
>= 75400 psi
H.C. Starck HPM 1800 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Tensile Strength, Yield >= 520 MPa
>= 75400 psi
H.C. Starck HPM 1801 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Tensile Strength, Yield >= 520 MPa
>= 75400 psi
H.C. Starck HPM 1810 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Tensile Strength, Yield >= 520 MPa
>= 75400 psi
H.C. Starck HPM 1850W Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Tensile Strength, Yield >= 520 MPa
>= 75400 psi
H.C. Starck HPM 1750 Tungsten High Density Composite Sheet
Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for further processing by the custo..
Tensile Strength, Yield >= 520 MPa
>= 75400 psi
H.C. Starck HPM 1751 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Tensile Strength, Yield >= 520 MPa
>= 75400 psi
H.C. Starck HPM 1850 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Tensile Strength, Yield 520 MPa

@Strain 0.200 %,
Temperature 650 °C
75400 psi

@Strain 0.200 %,
Temperature 1200 °F
Precipitation Hardened prior to test
Special Metals NIMONIC® Alloy 81
A precipitation-hardenable nickel-chromium alloy with enhanced resistance to high-temperature corrosion. The excellent hot-corrosion resistance of the alloy results from its high chromium content o..
Tensile Strength, Yield 520 MPa
75400 psi
Elgiloy® Co-Cr-Ni Alloy, Strip
General Elgiloy® information: High strength, ductility, fatigue life, and good mechanical properties. Corrosion resistant in numerous environments. Available in strip (currently 0.0015" to 0.075"..
Tensile Strength, Yield 520 MPa

@Strain 0.200 %
75400 psi

@Strain 0.200 %
ATI Allegheny Ludlum AL 29-4C® Stainless Steel, UNS S44735
AL 29-4C alloy is a superferritic stainless steel designed by Allegheny Ludlum for extreme resistance to chloride ion pitting, crevice corrosion and stress corrosion cracking, as well as general cor..