Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 515 MPa | >= 74700 psi | |
MetalTek MTEK 2507 Cast UNS J93404 Duplex Stainless Steel Excellent seawater corrosion resistance combined with nearly twice the strength of common stainless steels.Applications: Offshore piping systems, couplings. Centrifuge, dewatering equipment. Pump, v.. |
|||
Tensile Strength, Yield | 515 MPa @Strain 0.200 %, Temperature 760 °C |
74700 psi @Strain 0.200 %, Temperature 1400 °F |
|
Haynes 263® alloy, cold rolled sheet, solution treated and aged Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle.. |
|||
Tensile Strength, Yield | 515 MPa @Strain 0.200 % |
74700 psi @Strain 0.200 % |
Typical; Annealed Plate |
ATI Allegheny Ludlum AL 2205™ Duplex Stainless Steel, Plate > 0.1875" Duplex Stainless Steel, UNS S31803 Ferromagnetic. The AL 2205 alloy is a nitrogen-enhanced duplex stainless steel alloy. The nitrogen serves to significantly improved the corrosion resistance of the alloy; especially in the welded c.. |
|||
Tensile Strength, Yield | 515 MPa @Strain 0.200 % |
74700 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum AL 2003™ Duplex Stainless Steel Characteristics: superior stress corrosion cracking resistance to Types 316 and 317, yield strength double that of conventional austenitic stainless steel, good corrosion resistance, good chloride s.. |