Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Oxford Polymers 604-I Polycarbonate/ABS Alloy Polycarbonate/ABS AlloyInformation provided by Oxford Polymers. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Polymer Resources NY66-IM2-[color]-H Impact Modified Nylon 66, Heat Stabilized Nylon 66, Superior Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. .. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Polymer Resources PC/TP-GP1-HF PC/Polyester Alloy, High Melt Flow High Melt Flow, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by .. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Polymer Resources PC/TP-GP2 PC/Polyester Alloy High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Ravago Manufacturing Americas Hybrid S464LGUV Acrylonitrile Butadiene Styrene + PC Alloy Available in North America UV Stabilizer Good Toughness Low Gloss RoHS Compliant Form: Pellets Processing Method: Injection Molding Automotive Specifications: Chrysler MS-DB300 CPN4352 Color:.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N2040ML Nylon 6 (Cond) Information provided by Ravago. |
|||
Tensile Strength, Yield | 51.7 - 117 MPa | 7500 - 17000 psi | Average value: 85.9 MPa Grade Count:32 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Ravago Manufacturing Americas Hybrid B2025IU Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Fiberfil® J-60/10 Polypropylene Homopolymer, 10% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D-638 |
Glastic 1125 Corrosion-Resistant Panels Glastic® Corrosion-Resistant Panels are ideal for applications where resistance to both flame, and the splash or spill of laboratory chemicals is important. Glastic® Grade 1125 is asbestos-fr.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® PCT1000 PC/PET Alloy PC/PET alloy with outstanding chemical resistance and impact strengthAll information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Techmer ES Elastoblend® PA6/6 HI BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedUl File Number: E157318Appearance: BlackProce.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Star Plastics PC/PBT7820 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Techmer ES HiFill® POM CO 0167 S1 LE Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: Copolymer and Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Techmer ES HiFill® POM CO 0167 S2 LE Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: Copolymer and Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Techmer ES HiFill® POM HO 0167 S1 Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: HomopolymerInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM 638 |
PlastxWorld CEVIAN® S3500 PC/ABS alloy Flame retarded PC/ABS Alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Total PSC 529 Polystyrene Polystyrene 529 is a medium flow crystal specially formulated for mar resistance. The easy to process crystal minimizes visual defects from ejection and automated part handling. Typical applications.. |
|||
Tensile Strength, Yield | 51.7 MPa @Thickness 3.17 mm |
7500 psi @Thickness 0.125 in |
|
TPI Porene® ABS-GA800 High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 51.7 - 54.9 MPa | 7500 - 7960 psi | ASTM D638M |
DSM Somos® ProtoGen™ O-XT 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC -2 DescriptionDSM Somos® ProtoGen O-XT 18120 is a liquid photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demonstrate diffe.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 1002 Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ASA 5946 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High HeatInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Clariant 6604-HSL Nylon 66, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Clariant ABS4500G30 ABS, 30% Glass Reinforced Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Clariant Renol PA2SP0023 Nylon 6, Impact and Flow Modified, ESD Protection Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers DIAMALOY 627 PC/Polyester Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Clariant Renol POMSP0001 Acetal Copolymer, Aramid Fiber, PTFE Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Asahi Kasei Thermylene® P-10FG-2100 10% Glass Fiber Reinforced Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
PolyOne Lubri-Tech™ 5209 S2 Natural A Acetal Copolymer, 9 Melt with Silicone