Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 503 MPa @Strain 0.200 % |
73000 psi @Strain 0.200 % |
|
Haynes Hastelloy® C-22® alloy, SMAW weld, 316L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Yield | 503 MPa | 73000 psi | |
Universal Wire Works 617 Nickel Alloy Welding Wire Alloy 617 is used for TIG and MIG welding of Inconel type alloy 617 and alloys of similar composition. Alloy 617 welds produce high stress-rupture strength in prolonged exposure to high temperatures.. |
|||
Tensile Strength, Yield | 503 - 552 MPa | 73000 - 80000 psi | 0.2% offset |
Eagle Brass 230 Red Brass, Extra Spring CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |
|||
Tensile Strength, Yield | 503 - 579 MPa | 73000 - 84000 psi | 0.2% offset |
Eagle Brass 240 Low Brass, Extra Spring CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib.. |
|||
Tensile Strength, Yield | 503 - 586 MPa | 73000 - 85000 psi | 0.2% offset |
Eagle Brass 425 Tin Brass 2%, Extra Hard Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Tensile Strength, Yield | 503 - 621 MPa | 73000 - 90000 psi | 0.2% offset |
Eagle Brass 519 Phosphor Bronzes 6%, Hard Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Tensile Strength, Yield | 503 - 579 MPa | 73000 - 84000 psi | 0.2% offset |
Eagle Brass 715 Copper Nickel 30%, Hard 715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co.. |
|||
Tensile Strength, Yield | 503 - 607 MPa | 73000 - 88000 psi | 0.2% offset |
Eagle Brass 725 Copper Nickel Tin, Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Tensile Strength, Yield | 503 - 627 MPa | 73000 - 91000 psi | 0.2% offset |
Eagle Brass 762 Nickel Silver 12%, 3/4 Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |