Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 50.0 MPa | 7250 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ PPC-20G Black Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS (Europe-Africa-Middle East) CYCOLOY C6200 is a non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs. C6200 has improved processing window and edge crac.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® MC1300 PC+ABS Cycoloy MC1300 resin is an injection moldable PC/ABS blend with excellent flow and impact performance. It is designed for plating applications mostly used in the automotive industry. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics GELOY XP4025 ASA (Europe-Africa-Middle East) GELOY XP4025 is a high heat modified ASA/PC blend, for automotive exterior applications. It shows very good properties, gloss and colour retention, as well as faster cycle time over competitive mate.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 50 mm/min; ISO 527-1,2 |
Qualchem Danamid AFES-21 Polyamide 66 Impact resistant, dryInformation provided by Qualchem Zrt. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy FXTW30CP ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 5 [mm/min], Test Speed 50 [mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® S31 (3484) PA 6.10 Conditioned
(discontinued **) A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | cond.; ISO 527-1, -2; 50 mm/min |
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, halogen free flame retardant.Information provided by LANXESS. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® HX215HP PBT High Flow, Unreinforced, Polybutylene Terephthalate (PBT). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food conta.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® HX3061HP PBT PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity: 250C at 21.6 kgf is 1450-1850 poise. Available in Natural color (1001) only. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LX-0971 S ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | ISO 527 type 1 A |
Solvay TECHNYL® A 205F PA66, Conditioned Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Asia Pacific) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® K3501 PBT (Europe-Africa-Middle East) Unfilled PBT, Hydrollytically Stable, Heat Stabilized, Impact Modified. A hydrollytically stable grade designed for improved performance under heat/humidity environments. Targeted at automotive unde.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL ENV105 PPE+HIPS (Europe-Africa-Middle East) NORYL ENV105 is an impact modified extrusion grade with a Vicat B/120 of 115C according ISO 306. |
|||
Tensile Strength, Yield | 50.0 MPa @Strain 50.0 % |
7250 psi @Strain 50.0 % |
ISO 527 |
A. Schulman FORMION™ FI 131E Adhesive, Extrusion Grade DescriptionFormion® FI 131E is an adhesive grade extrusion product. It has been formulated to provide adhesion as a tie layer or resin modifier to bond Ionomer to polar and non polar substances, s.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | ISO 527 |
Polyram PlusTek PB340S50 Nylon 6 for Injection Molding, 50% Glass-beads Reinforced, Heat Stabilized 50% Glass-beads reinforced, heat stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | ASTM D638 |
Eastman Provista MP001 Copolymer Provista Copolymer MP001 is a resin specifically developed for extrusion into profiles where aesthetics such as high clarity and gloss, coupled with design flexibility, drive demand. Compared to com.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | dry; ISO 527-1/-2 |
DSM Akulon® Fuel Lock FL-LP PA6 Low fuel permeation PA6 suitable for use in injection molding/welding of small engine fuel tanks, UV stabilized |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® 2S 20 nat PA610 Product Description: Grilamid 2S 20 natural is an unmodified medium viscosity polyamide 610 (PA610), designed for injection molding as well as extrusion. It is characterized by the following product.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSS/4 LF 1 PA666 Product description: Grilon TSS/4 LF 1 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 1% lubricant (molybdenum disulphide). Grilon TSS/4 LF 1 has the following import.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSS/4 PA666 Product description: Grilon TSS/4 is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS/4 has the following important properties: Good flow behaviorEas.. |
|||
Tensile Strength, Yield | 50.0 MPa @Temperature 23.0 °C |
7250 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® CE2056 NC010 PBT Crastin® CE2056 NC010 is an unreinforced polybutylene terephthalate molding resin.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 50 mm/min; ISO 527 |
Chi Mei Wonderloy® PC-385 PC/ABS Alloy Ultra-high Heat, Ultra-high Impact |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437G30CL Glass Reinforced Coupled |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | ISO 527-1 |
Barlog Plastics KEBALLOY EP 23 ABS/PC, unreinforced, electro platable grade ABS+PCInformation provided by BARLOG plastics GmbH. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 50 mm/min; ISO 527 |
CP-Polymer-Technik Wellamid® 6000/58 CP Nylon 6, Impact Modified Until -40°C, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | ISO 527 |
Polyram RamShine PAS703 ASA, UV Stabilized Is a general purpose injection molding ASA, good chemical resistance, UV stabilization.Information provided by Polyram. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Europe-Africa-Middle East) PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | Conditioned; ISO R 527 |
Addiplast Addinyl B2 Nylon 6 Unreinforced, medium viscosityInformation provided by Addiplast. |