Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 5.90 MPa | 856 psi | M100 |
3M Dyneon™ Fluorel™ FC-2120 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Dipolymer for difficult extrusions. .. |
|||
Tensile Strength, Yield | 5.90 MPa | 856 psi | M100 |
3M Dyneon™ Fluorel II™ FX-11900 Fluoroelastomer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 59%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Good metal a.. |
|||
Tensile Strength, Yield | 5.90 MPa | 856 psi | Conductive Layer |
Fujipoly Industries Zebra® 1002 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tensile Strength, Yield | 5.90 MPa | 856 psi | Conductive Layer |
Fujipoly Industries Zebra® 1002 Carbon Sponge Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tensile Strength, Yield | 5.90 MPa | 856 psi | Conductive Layer |
Fujipoly Industries Zebra® 2004 Carbon Sponge Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tensile Strength, Yield | 5.90 MPa | 856 psi | Conductive Layer |
Fujipoly Industries Zebra® 2005 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tensile Strength, Yield | 5.90 MPa | 856 psi | Conductive Layer |
Fujipoly Industries Zebra® 2005 Carbon Sponge Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tensile Strength, Yield | 5.90 MPa | 856 psi | Conductive Layer |
Fujipoly Industries Zebra® LT 200 Low Temperature Carbon Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tensile Strength, Yield | 5.90 MPa | 856 psi | Conductive Layer |
Fujipoly Industries Zebra® 2004 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tensile Strength, Yield | 5.90 MPa | 856 psi | 100% elongation; ASTM D412 |
Lubrizol Estane® 5712 Thermoplastic Polyurethane Type: Estane® 5712 is a Polyester thermoplastic polyurethane (TPU).Feature: It has the highest peel and green strengths and shortest open-tack time of any Estane TPU resin used in adhesives. Suppl.. |
|||
Tensile Strength, Yield | 5.90 MPa | 856 psi | |
Dow AFFINITY™ SM 1300 Polyolefin Plastomer AFFINITY® SM 1300 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in high clarity durable injection molded industrial and consumer goods and compression molded closu.. |
|||
Tensile Strength, Yield | 5.90 MPa | 856 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8440 Polyolefin Elastomer Description: Engage® 8440 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It is an excellent thermoplastic elastomer .. |
|||
Tensile Strength, Yield | 5.90 MPa @Strain 50.0 % |
856 psi @Strain 50.0 % |
50 mm/min |
Arkema Group Pebax® MX 1059 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) Hardness 35 shore D Good resistance to oils. Applications: Automotive, cable...ISO data provided by the manufacturer, Arkema. |
|||
Tensile Strength, Yield | 5.90 MPa @Strain 100 % |
856 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® 1185A10W Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |