Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 5.83 MPa | 846 psi | 200%, post cured- 8 hours at 177°C; ASTM D412 |
Multibase C6-570 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 5.83 MPa | 845 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 3541 Clear TPE Thermoplastic Elastomer This material bonds to polypropylene.Forms:PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Tensile Strength, Yield | 5.83 MPa | 845 psi | AVG Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 5725 Fluorocarbon-Elastomer Formulated Viton®. General service.Information provided by Seals Eastern, Inc. |