Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 5.00 MPa | 725 psi | ASTM D412 |
Polymax® Maxelast® A9855B TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | ISO 527 |
Polimeri Europa Clearflex® MP D0 Very Low Density Polyethylene Clearflex MP D0 is a linear polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin shows an excellent balance between flexibility and impact resistance.Main Applicati.. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | ASTM D412 |
Precision Polymer Engineering E70Z Ethylene Propylene Rubber Peroxide cured, grey Ethylene Propylene Terpolymer, 65-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Specially formulated for sealing applications involving high voltage electri.. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | 50% Elongation; ASTM D412 |
Covestro Texin® DP7-3008 Thermoplastic Polyurethane, Polyester-based, Aliphatic
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | ASTM D638 |
Petroquimica Triunfo Tritheva® TN 8093 EVA Copolymer The Tritheva TN 8093 resin is a fractional MI copolymer of Ethylene-Vinyl Acetate (EVA), developed to meet the multi-layer and blending film applications where are required high strength, with high .. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | 150°C for 1,000 hrs; JIS-K-6251 |
Fujipoly Industries Sarcon® 25G-Td Thin-Film GR-TD Sarcon 25G-Td is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | ISO 527-1, -2 |
LyondellBasell Adflexâ„¢ Q 100 F Polyolefin Description: Adflexâ„¢ Q 100 F is a thermoplastic polyolefin which has been developed for the extrusion of blown film, it is also suitable for sheet extrusion. Adflexâ„¢ Q 100 F features a ver.. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | Elastic Limit |
Wolf Kunststoff ZEDEX® ZX-100EL63 A1G Polymer Alloy, Elastomer Modified Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol.. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | |
Trelleborg Commercial Neoprene® C722 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Tensile Strength, Yield | 5.00 MPa @Temperature 21.1 °C |
725 psi @Temperature 70.0 °F |
Flatwise Tensile; After 500 hrs at 400°F (Weight loss = 0.75%); Composite Honeycomb Sandwich Performance; ASTM C 297 |
Hexcel® Redux® HP655 Toughened BMI film Adhesive Redux® HP655 is a toughened BMI structural adhesive designed for metal to metal, composite to composite, and honeycomb sandwich bonding for both co-cured and precured composite skins. Redux® HP655.. |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 100 % |
725 psi @Strain 100 % |
ISO 527-1/-2 |
Covestro Desmopan® 3385A Polyurethane Extrusion- and injection molding gradegood wear resistanceshort cycle timeshigh melt stabilityApplicationhard - soft systemsHosesnon-reinforcedProfilesInjection molded engineering partsPreprocessing.. |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 100 % |
725 psi @Strain 100 % |
ISO 527-1/-2 |
Covestro Desmopan® 3485A Polyurethane Extrusion- and injection molding gradesuitable for extrusion blow moldingwith release agenthigh melt stabilityApplicationBellowsInjection molded engineering partsPreprocessingMax. Water content |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 100 % |
725 psi @Strain 100 % |
ISO 527-1/-2 |
Covestro Desmopan® 481 Polyurethane injection molding gradefree from plasticizersgrease and oil-resistantlow compression sethigh elasticitygood heat resistanceEasy releaseApplicationRoller coatingSealsmembranesAutomotive engineeringPr.. |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 100 % |
725 psi @Strain 100 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 1485A Polyurethane Extrusion- and injection molding gradesuitable for extrusion blow moldingvery large processing windowhigh melt stabilityBeadsApplicationBellowsHosesnon-reinforcedProfilesInjection molded engineering.. |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 300 % |
725 psi @Strain 300 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 1960AW Polyurethane As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 300 % |
725 psi @Strain 300 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 1970AW Polyurethane As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 100 % |
725 psi @Strain 100 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 8785 A Polyurethane injection molding gradewith special UV stabilizersEasy releaseshort cycle timesApplicationSports shoe solesPreprocessingMax. Water content |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 100 % |
725 psi @Strain 100 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 8785A S043 Polyurethane injection molding gradewith special UV stabilizersexcellent abrasion resistanceEasy releaseshort cycle timesApplicationSports shoe solesPreprocessingMax. Water content |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 50.0 % |
725 psi @Strain 50.0 % |
|
Covestro Texin® 285 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Baye.. |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 50.0 % |
725 psi @Strain 50.0 % |
|
Covestro Texin® 990R Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Baye.. |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 50.0 % |
725 psi @Strain 50.0 % |
50 mm/min |
Arkema Group Nakan® FKS 918 R PVC, Soft Extrusion Grade NAKAN FKS 918 R is a soft polyvinyl chloride compound developed for general insulation and sheathing.ISO data provided by the manufacturer, Arkema. |
|||
Tensile Strength, Yield | 5.00 MPa @Strain 50.0 % |
725 psi @Strain 50.0 % |
50 mm/min |
Arkema Group Nakan® FSS 601 R PVC, Soft Injection Molding Grade NAKAN FSS 601 R is a soft polyvinyl chloride compound developed for injection molding of transparent soling ( very clear ).ISO data provided by the manufacturer, Arkema. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | |
BASF Lucalen® A 3110 M Ethylene/Acrylate Copolymer Economical composite films together with PE-LD; primers for aluminum/steel composites; coatings for paper board, aluminum and steel (e.g. for pipes used to transport petroleum, gas, etc.)Data was co.. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | |
BASF Lucalen® A 3120 M Ethylene/Acrylate Copolymer Suitable in similar manner as Lucalen A 2920 M or also as a material for coating aluminum, steel, paper and cardboard. Also for processing pipes for transporting petroleum, gas, etc.Data was collec.. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | |
ACC MM240T Addition Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: cures at room temperature, low shrinkage, high tear and tensile strengths. Applications: rapid prototyping. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | |
ACC MMAD25 Addition Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: cures at room temperature, low viscosity, low shrinkage, high tear and tensile strengths. Applications: plaster casti.. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | 50 mm/min |
Arkema Group Evatane® 1040 VN 4 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for flexible films with high transparency and high mechanical properties. Examples: thin stretch film for food packaging, coex.. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | ASTM D638 |
ExxonMobil Escorene® LD-728 High EVA Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Applications: Injection molding; Foams.. |
|||
Tensile Strength, Yield | 5.00 MPa | 725 psi | ASTM D638 |
ExxonMobil Escorene® LD-730 High EVA Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Applications: Injection molding; Foams.. |