Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 48.3 MPa | 7010 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ AT-000/05T Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 48.3 MPa | 7010 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Novablend™ 5035 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Polymer Resources TP-GP1 Polybutylene Terephthalate, General Purpose, Flow Modified Polybutylene Terephthalate, General Purpose, Flow ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Polymer Resources AC-G10 Acetal Copolymer, 10% Glass Reinforced Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 48.3 MPa | 7010 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® AT-000/000 HI5 Natural NA Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ AT-000/8T Acetal-Copolymer, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
PolyOne Stat-Tech™ AS-10NCF/000 ABS - 10% Nickel Coated Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Yield | 48.3 MPa | 7010 psi | |
Ineos ABS Lustran® 248 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | |
Lord Adhesives Circalokâ„¢ 6009 A/B Flame Retardant Epoxy Encapsulant Circalokâ„¢ 6009 A/B is a two component epoxy resin system which has moderate thermal conductivity and low viscosity. Circalokâ„¢ 6009 A/B meets UL 94V-0 specification for flame retardance.All.. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Fiberfil® J-61/20/E Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6 FR IM BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedAppearance: BlackTPCI# 9993101Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Techmer ES HiFill® HDPE GF10 CC 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Techmer ES HiFill® HDPE GF30 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Techmer ES HiFill® POM CO 0241 S Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Techmer ES HiFill® PP GF/M40 CC BK 40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Techmer ES Luriblend® POM HO TL20 BN042 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated and HomopolymerAppearance: Brown, Natural Color and RedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Techmer ES Plastiblend® PC/PBT IM 5720 A BK Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Techmer ES Plastiblend® PPS/F 0328 Availability: North AmericaForms: Pellets Additive: Lubricant and Strontium Ferrite Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Techmer ES Statiblend® PA12 CB Availability: North AmericaForms: PelletsAdditive: Carbon BlackFeatures: ConductiveAppearance: BlackTPCI# 9872105Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 48.3 MPa | 7010 psi | ASTM Data |
Styron Magnum™ 9010 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Techmer ES HiFill® PA4/6 GF5 IM HS BK 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact Modifie.. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Techmer ES HiFill® PBT 0158 S Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 48.3 MPa @Thickness 3.17 mm |
7000 psi @Thickness 0.125 in |
ASTM D638 |
Samsung Cheil Industries Starex® SR-0300 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | ASTM D638 |
Westlake Plastics Kynar® 740 PVDF Homopolymer Manufactured from Kynar® polyvinylidene fluoride resin. This material offers excellent corrosion and chemical resistance at both ambient and elevated temperatures, PVDF is also inherently UV stab.. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 2510 Description: Injection Molding Grade, Medium Impact, Super High FlowInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | TM R050-36 |
Resinlab® EP691 Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP691 is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting and ad.. |
|||
Tensile Strength, Yield | >= 48.3 MPa | >= 7000 psi | ASTM D638 |
Buckeye Polymers BP RPP 3009 GK BLK Polypropylene, Glass Filled Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced en.. |
|||
Tensile Strength, Yield | 48.3 MPa | 7000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AT-10GB/000 Acetal-Copolymer, Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 48.3 MPa | 7010 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® XT XT-100-CX02-EG PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |