Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 464 MPa @Strain 0.200 %, Temperature 538 °C |
67300 psi @Strain 0.200 %, Temperature 1000 °F |
|
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 15.9 mm thick bar Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Tensile Strength, Yield | 464 MPa @Strain 0.200 % |
67300 psi @Strain 0.200 % |
statistical analysis gives AVG-3STD at 417 MPa |
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Forged Plate Aluminium alloy 2124 reinforced with 25 volume % silicon carbide particles (average size 3 micron). It is manufactured by a powder metallurgy route using high-energy mixing to ensure excellent part.. |