Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 45.9 MPa | 6660 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging 2797 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 45.9 MPa | 6660 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging XPL319 Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of.. |
|||
Tensile Strength, Yield | 45.9 MPa | 6660 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Dry Blend E6530 Polyvinyl Chloride, Rigid (PVC, Rigid) Interior application for thick & thin gauge profile application.Information provided by PolyOne |
|||
Tensile Strength, Yield | 45.9 MPa | 6660 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Dry Blend E7364 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |