Mechanical Properties Metric English Comments
Tensile Strength, Yield 43.8 MPa
6350 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging 2210 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Strength, Yield 43.8 MPa
6350 psi
50mm/min; ISO 527
Styron Magnumâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS)
High Heat, Low Gloss ABS.Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.