Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 43.4 MPa | 6290 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging 161J-1-3V/2188GC-3V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 87850 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M3890 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D638 |
Omni Plastics OmniTuff™ CPP GRC10 Copolymer Polypropylene Glass Reinforced Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni.. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | |
Parylene Coating Services N Poly (P-Xylylene) Monomer is para-xylylene. Parylene N has a lower coefficient of friction and therefore is recommended where lubricity is needed. Parylene N exhibits a slight haze at thicknesses over 5 microns.Par.. |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Dry Blend E7506 Polyvinyl Chloride, Rigid (PVC, Rigid) Geon E7506 is recommended for whites and light pastel colors only. Performs well in extrusion blow molding and high rate fencing capstock applications.Physical properties based on Geon E7506 white 1.. |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Dry Blend E7755 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
PolyOne Stat-Tech™ NJ-10SS/000 Nylon 12 - 10% Stainless Steel Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D638 |
Global GP-150 High Impact Polystyrene High flowGood stiffnessApplications:AppliancesElectrical/Electronic applicationsHousehold goodsFood packagingToys |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM-D638 |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Tensile Strength, Yield | 43.4 MPa @Temperature 23.0 °C |
6290 psi @Temperature 73.4 °F |
ASTM D638 |
IRPC Polimaxx Polene GP150 Polystyrene APPLICATIONS: INJECTION MOULDING ELECTRICAL APPLIANCES, HOUSEHOLD PRODUCT, TOYS, SANITARY WARE, etc. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D638 |
Techmer ES Plastiblend® ABS/PBT 1500 Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D638 |
Techmer ES Plastiblend® PA6 SF80 L Availability: North AmericaForms: Pellets Additive: Lubricant and Strontium Ferrite (80%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D638 |
Techmer ES Plastiblend® PBT/ABS BK Availability: North AmericaForms: PelletsAppearance: BlackTPCI# 6722121Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | ASTM Data |
Styron Magnum™ 555 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | ASTM Data |
Styron Magnum™ 585 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | ASTM Data |
Styron Magnum™ 9015 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | ASTM Data |
Styron Magnum™ 9700HF ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D638 |
Star Plastics ABS3545 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | 105% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Calcium Chloride aq. for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 3001MC Description: Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 3002MC Description: Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS TS-12 Injection Molding Grade, Medium Heat Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D-638 |
Axiall 7777 Rigid PVC, Extrusion Georgia Gulf 7777 is a rigid PVC compound designed for outdoor applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D-638 |
Axiall 9209 Rigid PVC, Molding Georgia Gulf 9209 is a food grade compound containing excellent optical and processing characteristics. It is suitable for use in a variety of food, cosmetic and general purpose packaging applicati.. |
|||
Tensile Strength, Yield | 43.4 - 90.3 MPa | 6300 - 13100 psi | Average value: 75.3 MPa Grade Count:22 |
Overview of materials for Nylon 6, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D-638 |
Axiall 2651 Rigid PVC, Molding Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM 638 |
PlastxWorld CEVIAN® B45M0 PBT/ABS Alloy These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |