Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 43.0 MPa | 6240 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® FXS600AR ABS (Europe-Africa-Middle East) Visual Ares effect Cycolac ABS material with excellent flow properties. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics GELOY CR8510 ASA ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Geloy XTWM206 ASA Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Geloy FXTW26SK ASA (Asia Pacific) Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Asia Pacific region... |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ASTM D638 |
Chevron Phillips HiD® 9720 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear homopolymerCharacteristics: good flow, moderate impact strength, excellent stiffness, moderate ESCR, moderate shrinkage resistanceApplications: pails, structural foamInformation p.. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ISO R527 |
Fainplast Compounds RKS 205/K-UV Rigid PVC, Antishock Extrusion Lead Free Metal effect antishock UV resistant profiles |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | SABIC - Japan Method |
SABIC Innovative Plastics NORYL SE100P PPE+HIPS (Asia Pacific) |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP WL0049 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WL0049 is a compound based on Polybutylene Terephalate resin containing PTFE and Flame Retardant. Added features include: Internally Lubricated, Flame Retardant. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRILOY R2000A PA 66 (Asia Pacific) LNP LUBRILOY* R2000A is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® 6620 PBT+PC PBT+PC, Unreinforced, impact modified thermoplastic alloy. Outstanding impact at low temperature |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Asia Pacific) Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS (Asia Pacific) LNP* Stat-loy* AF306 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Antistat. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DF004P PC (Asia Pacific) LNP* Thermocomp* DF004P is a Polycarbonate base resin containing Glass Fiber. Characteristics of this grade are Exceptional Processing. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | 50mm/min; ISO 527 |
Styrolution Terblend® N NM-11 ABS/PA6 (Dry) Terblend N NM-11 is an ABS/PA6 blend combining very high impact strength, even at low temperatures, with an excellent processability and surface appearance.Information provided by STYROLUTION, which.. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP PH1100B PA 6 LNP* THERMOCOMP* PH1100B is a compound based on Nylon 6 resin. Added feature of this material is: High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP YF003S Polyester Elastomer (Europe-Africa-Middle East) LNP* THERMOCOMP* YF003S is a compound based on Polyester Elastomer containing Glass Fiber. Added features include; Heat Stabilized. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PVX524 PPE PREVEX* PVX524 resin is a high flow, non FR grade, 100 C HDT |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY KX96821 Acetal LNP STAT-LOY* KX96821 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Antistat. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Asia Pacific) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | SABIC - Japan Method |
SABIC Innovative Plastics Noryl EBN3001 PPE+HIPS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ASTM D638 |
Eastman Tritan MX710 Copolyester Eastman Tritan Copolyester MX710 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX710 has many outstanding features that include excellent toughness, hydr.. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ASTM D638 |
Eastman Tritan TX1000 Copolyester Eastman Tritan TX1000 is an amorphous copolyester with excellent appearance and clarity. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistanc.. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ASTM Data |
Dow Retain® ABS 7490 ABS Data provided by Dow Chemical. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | |
Fainplast Compounds R 220 Rigid PVC, Extrusion Rolling shutters |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | |
Fainplast Compounds R 316 Rigid PVC, Extrusion Rolling shutters |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | |
Fainplast Compounds R 316/AS Rigid PVC, Extrusion Antistatic profiles |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | ISO 527-2 |
Tisan TISOPLEN® 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL004XXC PC LNP* LUBRICOMP* DL004XXC is a compound based on Polycarbonate containing 20% PTFE. Characteristics of this grade are: Interrnally Lubricated. |