Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 410 - 560 MPa | 59500 - 81200 psi | |
Materion Beryllium Copper Alloy 25 Strip; 1/4 H (TD01) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): 0Superficial Hardness: 30T 62-75Tabulated properties apply .. |
|||
Tensile Strength, Yield | 410 MPa @Strain 0.200 % |
59500 psi @Strain 0.200 % |
|
Haynes 556® alloy, bar, after 1000 hours at 650°C (1200°F) Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Yield | 410 MPa @Strain 0.200 % |
59500 psi @Strain 0.200 % |
|
Haynes 556® alloy, bar, after 8000 hours at 650°C (1200°F) Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Yield | 410 MPa @Strain 0.200 % |
59500 psi @Strain 0.200 % |
|
Haynes 556® alloy, cold rolled, solution annealed sheet, 0.8-2.8 mm thick Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Yield | 410 MPa @Strain 0.200 % |
59500 psi @Strain 0.200 % |
Solution Annealed. Value at room temperature |
Special Metals NIMONIC® Alloy 86 A nickel-chromium-molybdenum alloy with a rare-earth (cerium) addition. It combines good formability and weldability with exceptional resistance to oxidation and scaling at temperatures to 1920°.. |
|||
Tensile Strength, Yield | >= 410 MPa | >= 59500 psi | |
AK Steel ASTM A 607 Class 1 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec.. |
|||
Tensile Strength, Yield | >= 410 MPa | >= 59500 psi | |
AK Steel ASTM A 607 Class 2 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. .. |
|||
Tensile Strength, Yield | >= 410 MPa | >= 59500 psi | |
AK Steel ASTM A 715 Class 2 Formable, Grade 60F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 715 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. .. |
|||
Tensile Strength, Yield | >= 410 MPa | >= 59500 psi | |
AK Steel SAE J1392, Grade 60F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) AK Steel Formable Grade - F indicates inclusion controlled low alloy.Information provided by AK Steel |
|||
Tensile Strength, Yield | 410 - 450 MPa | 59500 - 65300 psi | L direction |
ArcelorMittal Save 20-13 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 410 - 450 MPa | 59500 - 65300 psi | T direction |
ArcelorMittal Save 20-15 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 410 - 450 MPa | 59500 - 65300 psi | L direction |
ArcelorMittal Save 25-14 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 410 - 450 MPa | 59500 - 65300 psi | T direction |
ArcelorMittal Save 25-16 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 410 - 450 MPa | 59500 - 65300 psi | L direction |
ArcelorMittal Save 27-15 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 410 - 450 MPa | 59500 - 65300 psi | T direction |
ArcelorMittal Save 27-17 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 410 - 450 MPa | 59500 - 65300 psi | L direction |
ArcelorMittal Save 30-15 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 410 - 450 MPa | 59500 - 65300 psi | T direction |
ArcelorMittal Save 30-17 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 410 - 510 MPa | 59500 - 74000 psi | |
ArcelorMittal TRIP 690 Very high strength steel, Cold Rolled Steel Available in the following: uncoated (HCT690T), electrogalvanized (HCT690T+ZE) and Extragal®/Galvannealed (HCT690T+Z)Description: TRIP steels offer an outstanding combination of strength and ductil.. |
|||
Tensile Strength, Yield | >= 410 MPa | >= 59500 psi | |
AK Steel ASTM A 1011, Class 2 Formable, Grade 60F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA-F) Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 410 MPa | >= 59500 psi | |
AK Steel ASTM A 1011, Class 2 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |