Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical AF342F ABS, Flame Retardant, High Flow Feature: Injection Molding, Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided .. |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical HIPS MI730 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUCEL HI520 POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical AF308 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® AS-0151 ABS, Unreinforced Anti-staticInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® CR-0760 ABS, Unreinforced Good chemical resistanceInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® GC-0770 H ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® NH-1904 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SP-0183 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® TX-0530T TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VH-0800 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® AS-0151 ABS, Unreinforced Anti-staticInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® GC-0770 H ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® NH-0825 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® TX-0530T TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VH-0800 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | ASTM D638 |
SCG Chemicals EL-Proâ„¢ P702J Polypropylene Injection Molding Key Characteristics:High clarityHigh stiffnessGood processabilityMicrowavable for cooking applicationsOdorlessSafe for food contactRecommended Applications:General purpose injection parts that requi.. |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron AN-450 Flame Retardant ABS Grade Information provided by Bhansali |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron IM-18 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
Type 1; ASTM D638 |
Bhansali Engineering Abstron MIF-45 ABS Injection Molding Grade High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron AN-450 EVM Flame Retardant ABS Grade Information provided by Bhansali |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron AN-450 Flame Retardant ABS Grade Information provided by Bhansali |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron IM-18 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Tensile Strength, Yield | 41.2 MPa | 5980 psi | |
ACC 1KSP EPI Engineered Polymers Silicone Polyurea Dispersion 1KSP is a silicone modified polyurea dispersion “Powered by ReactAmine® Technology” designed for a wide range of rigid and flexible substrates such as wood, metal, vinyl, concrete and other plast.. |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron AN-450 EVM Flame Retardant ABS Grade Information provided by Bhansali |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron MIF45EP ABS Injection Molding Grade Electroplating, High FlowInformation provided by Bhansali |
|||
Tensile Strength, Yield | 41.2 MPa | 5970 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SBF 3778 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact AcceptableUses: Shrink Wrap Forms: Pellets Processing Method: Blown FilmInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron MIF45EP ABS Injection Molding Grade Electroplating, High FlowInformation provided by Bhansali |
|||
Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron HCR-15 M ABS Heat Resistant Chemical Resistant GradeInformation provided by Bhansali |