Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 40.7 MPa | 5900 psi | ASTM D638 |
Multibase Multi-Pro® 1505 R Polypropylene Glass Fiber Reinforced, 15% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | ASTM D638 |
Multibase Multi-Pro® 4010 M Polypropylene Mica Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses:Pump PartsInformation provided by Multibase |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion LR620 white 1046 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | ASTM D638 |
Polymer Resources ABS-FR Flame Retardant ABS Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch.. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | ASTM D638 |
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized Flame Retardant Acrylonitrile Butadiene Styrene, UV-stabilizedFeatures: • Flame Retardant • Self Extinguishing • Good UV ResistanceProcess: Injection MoldingNotes: All physical, mechanical and.. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | ASTM D638 |
Polimeri Europa SINKRAL B532 ABS, Very High Impact
(discontinued **) Very high impact; injection/extrusion grade.Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | ASTM D638 |
Ravago Manufacturing Americas Hylac® GP48 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | ASTM D638 |
Techmer ES HiFill FR® ABS FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantTPCI# 1039121Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | ASTM D638 |
Techmer ES HiFill FR® ABS FR BK Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackTPCI# 9224121Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | ASTM D638 |
Techmer ES HiFill FR® ABS FR UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | ASTM D638 |
Techmer ES HiFill FR® ABS FR UV BK Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame Retardant and Good UV ResistanceUL File Number: E157318Appearance: BlackTPCI# 9224121Information provided by TP Compos.. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | ASTM D638 |
Techmer ES HiFill FR® ABS FR V2 BK Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | ASTM D638 |
Spartech Royalite R522 PVC Alloy Aircraft Grade Sheet Description: Aircraft Grade SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | ASTM D638 |
Spartech Royalite R60 PVC/Acrylic Aircraft Grade Sheet Description: Aircraft Grade SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | ASTM D638 |
Spartech Royalite R66 PVC/Acrylic Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | ASTM D638 |
Techmer ES HiFill FR® PA6 E FR Availability: North AmericaForms: PelletsFeatures: Flame Retardant Processing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | ASTM D638 |
Eastman Tenite 285E3720005 Butyrate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 7600B (ELG) Description: Blow Molding Grade, Extra High Impact, Low GlossInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS/PC 7901 Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers Centrex® 810 Injection Molding Grade Centrex 810 resin is a soft-flow, high-gloss, and medium-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and .. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | chs 50 mm/min; tangent; ASTM D638 |
Diamond Polymers NPP30-2000HC Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | ASTM D638 |
Eastman Tenite Propionate 358A4000018 Clear, Trsp Cellulose Acetate Propionate Plasticizer 8%. Weight loss on heating = 0.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | ASTM D-638 |
Axiall 9246 Rigid PVC, Molding Georgia Gulf 9246 is a high impact compound suitable for food packaging.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | ASTM D-638 |
Axiall 7407 Rigid PVC, Extrusion Georgia Gulf 7407 is a rigid PVC compound designed for outdoor applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | ASTM D-638 |
Axiall 7765 Rigid PVC, Extrusion Georgia Gulf 7765 is a general-purpose indoor rigid PVC profile extrusion compound designed for applications requiring the following properties. 7765 carries an NSF standard 51 listing (for food zo.. |
|||
Tensile Strength, Yield | 40.7 - 181 MPa | 5900 - 26200 psi | Average value: 114 MPa Grade Count:35 |
Overview of materials for Nylon 66, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Tensile Strength, Yield | 40.7 - 121 MPa | 5900 - 17500 psi | Average value: 62.8 MPa Grade Count:27 |
Overview of materials for Polycarbonate, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | ASTM D638 |
Polimeri Europa SINKRAL G523 ABS, High Impact
(discontinued **) High impact; good flow; high gloss.Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line. |
|||
Tensile Strength, Yield | 40.7 MPa | 5900 psi | ASTM D638 |
Spartech Royalite R60-LS (R61) PVC/Acrylic Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |